| PHASE BOUNDARY OF α_2 PRECIPITATION IN Ti-Al-La TERNARY SYSTEM |
| YANG Rui;LI Dong;WAN Xiaojing Institute of Metal Research; Academia Sinica; Shenyang |
|
Cite this article:
YANG Rui;LI Dong;WAN Xiaojing Institute of Metal Research; Academia Sinica; Shenyang. PHASE BOUNDARY OF α_2 PRECIPITATION IN Ti-Al-La TERNARY SYSTEM. Acta Metall Sin, 1988, 24(4): 288-290.
|
|
|
Abstract The phase boundary of α_2 precipitation at 600℃ in Ti-Al-La ternary systemhas been determined by TEM examination, which shows three kinds of phase regions, namelythe single α phase region, the transitional region where there is superlattice reflection but no α_2precipitation and the α+α_2 region. A point of maximum aluminium content was found to exist onthe α/α+a_2 boundary and the track of the boundary was explained in terms of the internal oxida-tion of lanthanum and the electron concentration rule for α_2 formation
|
|
Received: 18 April 1988
|
1 Rosenberg H W. In: Jaffee R I, Promisel N E eds., The Science, Technology and Application of Titanium. London: Pergamon, 1970: 851 2 李东,刘羽寅,万晓景.金属学报,1984;20:A375 3 李东,刘羽寅.金属学报,1984;20:A384 4 李东,万晓景.金属学报,1984;20:A391 5 Sastry S M L, O' Neal J E, Lederich R J, Rath B B. J Mater Sci, 1979; 14: 179 6 Sankaran K K. Sastry S M L, O' Neal J E. Metall Trans, 1980; 11A: 198 7 Blackburn M J. Trans Metall Soc AIME, 1967; 239: 1200 8 杨锐.硕士学位论文,中国科学院金属研究所,1987年4月 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|