Abstract Fracture behaviour of low-all oysteels AISI4340, HY100, WELTEN60, AISIA537 and A131 in artificial seawater under static, cyclic loading and cath-odic protection potential has been investigated by using fracture mechanics, elec-trochemistry and electronfractography. The results reveal that under hydrogen evo-lution potential (cathodic protection potential) the critical yield strength requiredfor the occurrence of SCC decreases from 985 to 872MPa comparing with corrosionpotential (E_c). The effect of cathodic protection on crack propagation of CF is notsimple, it is closely related to the yield strength of steels and their SCC behaviour.For the steels with high yield strength, cathodic protection promotes da/dN
|
|
Received: 18 April 1988
|
1 徐克薰,俞健,郑文龙.机械工程材料,1985;9(1) :1 2 Duquette D J, Uhlig H H. ASM Trans Q, 1968; 61: 449 3 #12 4 Hooper W C, Hartt W H. Corros, 1978: 34: 320 5 Hartt W H. Hooper W C. Corros, 1980; 36: 107 6 Scott P M, Silvester D R V. The Influence of Mean Tensile Stress on Corrosion Fatigue Crack Growth in Structural Steel Immersed in Seawater, ITR3/62, UK Offshore Steels Research Project, Proceeding of European Offshore Steels Research Seminar, London, May 25, 1977, III/p. 5-2 7 Hartt W H. ASTM STP761, 1982: 1--14 8 郑文龙,朱国培,欧阳怀谨,李革.金属学报,1986;22:275-281 9 National Association of Corrosion Engineers Standard TM-01-77, In: Mater Perform 1977; 16 (9) : 61p |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|