MECHANISM OF INOCULATION OF CAST IRON
QIN Ziqiang;YU Zongsen Beijing University of Iron and Steel Technology
Cite this article: 

QIN Ziqiang;YU Zongsen Beijing University of Iron and Steel Technology. MECHANISM OF INOCULATION OF CAST IRON. Acta Metall Sin, 1988, 24(1): 129-132.

Download:  PDF(935KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The "carbon peaks" and high carbon activity spots appear in molten cast ironduring inoculation by Si. No evidence shows that the number of Si-rich particles whichmight be the heterogeneous nuclei of graphite is increased by inoculation. It is suggested thatthe mechanism of inoculation is the undulation of C concentration and activity in an inocu-lated cast iron. The fading of inoculation is caused by the fading of undulation.
Key words:  cast iron      inoculation      catbon activity      electron      probe microanalysis     
Received:  18 January 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I1/129

1 Crank J. The Mathematics of Diffusion, Oxford, 1956; p. 12
2 Signarth G K. Met Sci, 1974; (8) : 298
3 Yeumann F, Dotsch E. In: Lux B et al. The Metallurgy of Cast Iron, Proc of the Symp, Geneva, 1974, 31
4 Loper C R, Heine R W, Chaudhari M D. In: Lux B et al. The metallurgy of Cast Iron Proc of the Symp. Geneva, 1974, 639
[1] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[2] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[3] DUAN Huichao, WANG Chunyang, YE Hengqiang, DU Kui. Electron Tomography Analysis on the Structure and Chemical Composition of Nanoporous Metal Surfaces[J]. 金属学报, 2023, 59(10): 1291-1298.
[4] HUANGFU Hao, WANG Zilong, LIU Yongli, MENG Fanshun, SONG Jiupeng, QI Yang. A First Principles Investigation of W1 - x Ir x Alloys: Structural, Electronic, Mechanical, and Thermal Properties[J]. 金属学报, 2022, 58(2): 231-240.
[5] WANG Shuo, WANG Junsheng. Structural Evolution and Stability of the δ′/θ′/δ′ Composite Precipitate in Al-Li Alloys: A First-Principles Study[J]. 金属学报, 2022, 58(10): 1325-1333.
[6] FAN Yongxia, WANG Jian, ZHANG Xuezhe, WANG Jianzhong, TANG Huiping. Mechanical Property of Shell Minimal Surface Lattice Material Printed by SEBM[J]. 金属学报, 2021, 57(7): 871-879.
[7] ZHOU Hongyu, RAN Minrui, LI Yaqiang, ZHANG Weidong, LIU Junyou, ZHENG Wenyue. Effect of Diamond Particle Size on the Thermal Properties of Diamond/Al Composites for Packaging Substrate[J]. 金属学报, 2021, 57(7): 937-947.
[8] CHEN Hongyu, SONG Xin, ZHOU Xianglong, JIA Wentao, YUAN Tao, MA Tianyu. Identification of 2:17R' Cell Edge Phase in Sm2Co17-Type Permanent Magnets by Transmission Electron Microscopy[J]. 金属学报, 2021, 57(12): 1637-1644.
[9] REN Dechun, ZHANG Huibo, ZHAO Xiaodong, WANG Fuyu, HOU Wentao, WANG Shaogang, LI Shujun, JIN Wei, YANG Rui. Influence of Manufacturing Parameters on the Properties of Electron Beam Melted Ti-Ni Alloy[J]. 金属学报, 2020, 56(8): 1103-1112.
[10] LIU Donglei, CHEN Qing, WANG De, ZHANG Rui, Tomiko Yamaguchi, WANG Wenqin. Formation and Friction Properties of Electron Beam Cladding (Ti, W)C1-x Composite Coatings on Ti-6Al-4V[J]. 金属学报, 2020, 56(7): 1025-1035.
[11] LI Gen, LAN Peng, ZHANG Jiaquan. Solidification Structure Refinement in TWIP Steel by Ce Inoculation[J]. 金属学报, 2020, 56(5): 704-714.
[12] Liqun CHEN, Zhengchen QIU, Tao YU. Effect of Ru on the Electronic Structure of the [100](010) Edge Dislocation in NiAl[J]. 金属学报, 2019, 55(2): 223-228.
[13] Xuemei XIANG, Yuxiang LAI, Chunhui LIU, Jianghua CHEN. Sn-Induced Modification of the Precipitation Pathways upon High-Temperature Ageing in an Al-Mg-Si Alloy[J]. 金属学报, 2018, 54(9): 1273-1280.
[14] Jing YU, Jijie WANG, Dingrui NI, Bolv XIAO, Zongyi MA, Xinglong PAN. Microstructure and Mechanical Properties of Additive Manufactured 2319 Alloy by Electron BeamFreeform Fabrication[J]. 金属学报, 2018, 54(12): 1725-1734.
[15] Xiuliang MA, Xiaobing HU. High-Resolution Transmission Electron Microscopic Study of Various Borides Precipitated in Superalloys[J]. 金属学报, 2018, 54(11): 1503-1524.
No Suggested Reading articles found!