INFLUENCE OF VACANCY TYPE DEFECTS ON REVERSE TRANSFORMATION AND SHAPE MEMORY EFFECT IN A Cu-Al-Zn-Mn-Ni ALLOY
by ZHAO Liancheng; YANG Jianhua; LIU Naihua; ZHANG Chunsheng;LEI Tingquan(Harbin Institute of Technology); GU Hua;HE Yongshu(Institute of High Energy Physics; Academia Sinica; Beijing)(Manuscript received 23 June; 1985; revised manuscript 10 January; 1986)
Cite this article: 

by ZHAO Liancheng; YANG Jianhua; LIU Naihua; ZHANG Chunsheng;LEI Tingquan(Harbin Institute of Technology); GU Hua;HE Yongshu(Institute of High Energy Physics; Academia Sinica; Beijing)(Manuscript received 23 June; 1985; revised manuscript 10 January; 1986). INFLUENCE OF VACANCY TYPE DEFECTS ON REVERSE TRANSFORMATION AND SHAPE MEMORY EFFECT IN A Cu-Al-Zn-Mn-Ni ALLOY. Acta Metall Sin, 1987, 23(5): 380-385.

Download:  PDF(1589KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  High temperature microscope, scanning electron microscope and positron annihilation techniques have been used to study the influence of vacancy type crystalline defects on reverse martensite transformation and shape memory effect in a Cu-Al-Zn-Mn-Ni alloy. Experimental results indicate that by decreasing cooling medium temperature, the reverse transformation is shifted to higher temperatures and completed in a wider temperature range, and the maximum shape recovery ratio is correspondingly decreased. But decreasing cooling medium temperature further to below a certain point will then result in a lower reverse transformation temperature and a narrower temperature range of completion, and a higher maximum shape recovery ratio. Some anomaly is observed when the specimen is quenched into A_f-M_f range. The experimental results are well explained according to the average life time τ and Doppler broadening line-shape parameter S of positron annihilation as well as the analysis of microstructure.
Received:  18 May 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I5/380

1 Humbeeck J V, Janssen J, Mwamba-Ngoie, Delaey L. Scr Metall, 1984; 18: 893
2 Delaey L, Suzuki T, Humbeeek J V. Scr Metall, 1984; 18: 899
3 赵连城,孙东立,雷廷权.金属学报,1983;19:A271
4 赵连城,杨建华.金属学报,1985;21:A 268
5 Siegal R W. Proc 6th Int Conf Positron Annihilation, 1982: 351
6 Yang J H, Zhao L C, Zhang C S, Lei T C. Scr Metall, 1987: 21 (3)u
No related articles found!
No Suggested Reading articles found!