| FORMATION MECHANISM OF BUTTERFLY MARTENSITE |
| by GONG Hai (Dalian Institute of Railway); GU Nanju (Hebei Technological Institute; Shijiazhuang)(Manuscript received 28; February;1986) |
|
Cite this article:
by GONG Hai (Dalian Institute of Railway); GU Nanju (Hebei Technological Institute; Shijiazhuang)(Manuscript received 28; February;1986). FORMATION MECHANISM OF BUTTERFLY MARTENSITE. Acta Metall Sin, 1987, 23(5): 374-379.
|
|
|
Abstract The butterfly martensite formed in T12A, GCr18Mo, CrMn and 25Cr2Ni-4WA (carburized) steels have been examined using optical microscopy and TEM. It was found that the mid-rib of butterfly martensite is a thin plate martensite and the formation of butterfly martensite is not a continuous process, but rather a compound one consisting of some separated stages. In the initial stage, the crossed or kinked thin plate martensite forms, and then it grows toward cross-range into the butterfly martensite with or without tail.
|
|
Received: 18 May 1987
|
1 梅本実,田村今男.水曜会誌,1980;119:281 2 贡海,苏东升.金属热处理,1983;(1) :32 3 纪芬,贡海.理化检验(物理分册),1985;21(5) :11 4 梅本実,渡井康之,田村今男.日本金属学会会誌,1980;44:453 5 Brook R, Entwisle A R. J Iron Steel Inst. 1965; 203: 905 6 Umemoto M, Tamura I. Proc of ICOMAT-79, Cambridge (USA), 1979: 53 7 Tamura I. Proc of ICOMAT-76, Kobe(Japan), 1976: 5 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|