Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (5): 386-390    DOI:
Current Issue | Archive | Adv Search |
INTERPHASE PRECIPITATION IN LOW CARBON STEELS
by SHI Deke; SONG Xiaoping (Xi'an Jiaotong University)(Manuscript received 27 December; 1985; revised manuscript 15 September; 1986)
Cite this article: 

by SHI Deke; SONG Xiaoping (Xi'an Jiaotong University)(Manuscript received 27 December; 1985; revised manuscript 15 September; 1986). INTERPHASE PRECIPITATION IN LOW CARBON STEELS. Acta Metall Sin, 1987, 23(5): 386-390.

Download:  PDF(1771KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Various types of carbide precipitation have been observed in steel 10 and 20SiMnMo during isothermal transformation. It seems that two interphase precipitation processes may occur. One of them takes place at the temperatures between pearlite and Bainite transformation, it may be associated with massive transformation and occurs mainly through a random transfer of atoms across γ/α interphase. Another involves bainite transformation, Ledge-propagation mechanism is the dominant feature of interphase precipitation. Both of them have been observed by means of TEM determination.
Received:  18 May 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I5/386

1 Honeycombe R W K. Met Sci, 1980; 14: 201
2 石德珂,柴惠芬 谈育煦,胡奈赛.钢中粒状贝氏体的组织与性能,西安交通大学科技报告,1978-063
3 俞德刚,郑经紘,梁振峰,沈甫法。金属学报,1983;19:A369
4 李承基.金属热处理学报,1984;5(2) :1
5 #12
6 Swanson WD, Parr J G. J Iron Steel Inst, 1964; 202: 104
7 Roberts M J. Metall Trans, 1970; 1: 3287
8 Wilson E A. Scr Metall, 1978; 12: 961
9 Massalski TB. Metall Trans, 1984; 15A: 421
10 Aaronson HI, Plichta MR, Franti G W, Russell K C. Metall Trans, 1978; 9A:363o
No related articles found!