Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (4): 285-404    DOI:
Current Issue | Archive | Adv Search |
TEM STUDY OF SECONDARY CARBIDES PRECIPITATION IN LOW ALLOYED HIGH SPEED STEEL DURING TEMPERING
by DING Peidao; PAN Fusheng; ZHOU Shouze (Chongqing University) (Manuscript received 27 November; 1985; revised manuscript 16 July; 1986)
Cite this article: 

by DING Peidao; PAN Fusheng; ZHOU Shouze (Chongqing University) (Manuscript received 27 November; 1985; revised manuscript 16 July; 1986). TEM STUDY OF SECONDARY CARBIDES PRECIPITATION IN LOW ALLOYED HIGH SPEED STEEL DURING TEMPERING. Acta Metall Sin, 1987, 23(4): 285-404.

Download:  PDF(3372KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The precipitation of secondary carbides in low alloyed high speed steel W3-Mo,2Cr4VSi during tempering and the influonce of Si, containing 0.2-2.3%, upon it were observed under TEM. It is shown that the disc-shaped carbide of MC-type, the ratio of thickness to diameter about 0.3-0.4, is the predominant finely dispersed secondary precipitate which is responsible for the peak hardness during tempering at 560℃. The orientation between MC carbide and matrix is found to be fulfilled the Baker-Nutting's relation: {010}_(MC)//{010}_α, <001>_(MC)//<101>_α The MC carbide is made fine during tempering at 560℃ when Si is added to steel, and the coarse M_6C carbide accelerated to precipitate along martensite boundary at 650℃. The MC morphology and the effect of Si on the precipitation of MC carbide are also discussed.
Received:  18 April 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I4/285

1 Andren H-O. Scr Met, 1981; 15: 749-752
2 Stiller K, Svensson L-E, Howell P R et al. Acta Metall, 1984; 32: 1457-1467
3 #12
4 潘复生,重庆大学,金属材料专业,硕士学位论文,1985
5 Kuo Kehsin (郭可信). J Iron Steel Inst, 1953; 174: 223
6 雍岐龙,郑鲁.金属学报.1984;20:A9-16
7 林栋梁,金属学报,1978;14:323
8 Bungardt K, Haberling E, Rose A. DEW-Tech Ber, 1972; 12: 111-133
9 Wriedt H A, Turkdogan E T.Met Sci, 1984; 18: 27-30
10 Zener C. J Appl Phys, 1949; 20: 950
11 #122
No related articles found!