Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (4): 291-298    DOI:
Current Issue | Archive | Adv Search |
THE NONEQUILIBRIUM CHARACTERISTIC OF BORON SEGREGATION AT AUSTENITE GRAIN BOUNDARIES DURING ISOTHERMAL HOLDING
by HE Xinlai; CHU Youyi; TANG Li; ZHOU Zhenxin; KE Jun (Beijing University of Iron and Steel Technology) (Manuscript received 20 June; 1985; revised manuscript 11 January; 1986)
Cite this article: 

by HE Xinlai; CHU Youyi; TANG Li; ZHOU Zhenxin; KE Jun (Beijing University of Iron and Steel Technology) (Manuscript received 20 June; 1985; revised manuscript 11 January; 1986). THE NONEQUILIBRIUM CHARACTERISTIC OF BORON SEGREGATION AT AUSTENITE GRAIN BOUNDARIES DURING ISOTHERMAL HOLDING. Acta Metall Sin, 1987, 23(4): 291-298.

Download:  PDF(1599KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The behaviour of grain bondary segregation and precipitation of B in B-bearing low C Mn-Mo steels and Fe-30%Ni alloys during isothermal holding has been investigated with particle tracking autoradiography. Specimens were quenched from 1350 or 1200℃ then isothermally held at 550—1000℃ for different periods. It is shown that the nonequilibrium grain boundary segregation pf B occurs as a dynamic process and the magnitude of it could be many times as large as that of equilibrium segregation. After cooling from the higher temperature, the B segregation, which is probably brought there by the complex of B atoms with supersaturated vancancies, increases at first with time, then upon the annihilation of vacancies, it becomes supersaturated with respect to equilibrium segregation concentration and thus decreases by diffusing back into the grains, giving a peak on the degree of segregation-holding time curve. The height and position of the peak depends on the initial heating and subsequent holding temperature. On the otherhand, if the holding temperature is lower, the nonequilibriumly segregated B becomes supersaturating and will precipitate at the grain boundaries, giving a curve increasing at first stage and then reaching a steady segregation. Thus, three kinds of grain boundary segregation kinetic curves are obtained at different isothermal temperatures.
Received:  18 April 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I4/291

1 Aust K T, Hanneman R E, Niessen P, Westbrook J H. Acta Metall, 1968; 16: 291
2 Harries D R, Marwick A D. Philiops Trans R Soc London, 1980; A 295: 197
3 Williams T M, Stonecham A M, Harries D R. Met Sci, 1976; 10: 14
4 Faulkner R G. J Mater Sci, 1981; 16: 373
5 贺信莱,褚幼义,张秀林,佘宗森,李秋萍,尹熙光.金属学报,1977;13:235
6 贺信莱,褚幼义,柯俊.金属学报,1982;18:1
7 贺信莱,褚幼义,柯俊.金属学报.1982;18:11
8 贺信莱,褚幼义,柯俊.金属学报,1983;19:A459
9 Karlsson L, Norden H. Proc JIMIS-4 Suppl to Trans Jpn Inst Met, 1986; 27: 189
10 He X L (贺信莱), Chu Y Y (褚幼义). J Phys D: Appl Phys, 1983; 16: 1145
11 褚幼义,贺信莱,唐立,徐庭栋,柯俊.金属学报,1987;23:169
12 Veno M, Jnoue T. Trans Iron Steel Inst Jpn, 1973; 13: 210
No related articles found!
No Suggested Reading articles found!