Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (4): 280-401    DOI:
Current Issue | Archive | Adv Search |
PRECIPITATION IN Ni-Ti ALLOY AND ITS INFLUENCE ON PROPERTIES
by ZHANG Yi; JIN Haling (Shanghai Iron and Steel Research Institute) (Manuscript received 7 April; 1986; revised manuscript 21 July; 1986)
Cite this article: 

by ZHANG Yi; JIN Haling (Shanghai Iron and Steel Research Institute) (Manuscript received 7 April; 1986; revised manuscript 21 July; 1986). PRECIPITATION IN Ni-Ti ALLOY AND ITS INFLUENCE ON PROPERTIES. Acta Metall Sin, 1987, 23(4): 280-401.

Download:  PDF(2510KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The formatiin rule of precipitation in Ni-rich, containing 51.6 at.-%Ni, NiTi alloy and its influence on properties have been investigated by means of observation under TEM and measurements of temperature dependence of resistivity, stress-strain curve and microhardness. The precipitate may be formed by aging at 300—600℃ and grown up with the increase of aging temperature and time. It Influences remarkably the shape-memory properties of the alloy.
Received:  18 April 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I4/280

1 Kolomytsev V I, Lobodyuk V A, Khandros L G. Phys Status Solidi, 1981; 65: 87
2 #12
3 张一,金嘉陵.金属学报,1985;21:A365
4 Nishida M, Wayman C M, Honma T. Scr Metall, 1984; 18: 1389
5 Nishida M, Wayman C M, Honma T. Scr Metall, 1985; 19: 983
6 Miyazaki S, Otsuka K. Metall Trans, 1986; 17A: 53
No related articles found!
No Suggested Reading articles found!