Please wait a minute...
Acta Metall Sin  1987, Vol. 23 Issue (3): 188-194    DOI:
Current Issue | Archive | Adv Search |
VARIATION OF Sb CONCENTRATION IN MELT DURING GROWTH OF HEAVILY Sb-DOPED Si SINGLE CRYSTAL
SHE Siming; CHENG Jun (Central South University of Technology; Changsha) (Manuscript received 13 January; 1985; revised manuscript 21 December; 1985)
Cite this article: 

SHE Siming; CHENG Jun (Central South University of Technology; Changsha) (Manuscript received 13 January; 1985; revised manuscript 21 December; 1985). VARIATION OF Sb CONCENTRATION IN MELT DURING GROWTH OF HEAVILY Sb-DOPED Si SINGLE CRYSTAL. Acta Metall Sin, 1987, 23(3): 188-194.

Download:  PDF(495KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A mathematical model has been established for the character of the variation of Sb concentration in the melt during the growth process of heavily Sb-doped Si single crystal. The calculated curve drawn with the model is in good agreement with the experimental one. As a result of the segregation of the solute during pulling, the concentration of Sb in the melt increases. It is found from the calculated curves that the increase of Sb concentration can be brought under control while the pulling process was carried out under a reduced pressure. Thus, the formation of cellular interface could be postponed. As the pressure in a furnace decreases to 2.7 kPa, the Sb concentration will be kept almost unchanged.
Received:  18 March 1987     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1987/V23/I3/188

1 Hurle D T J. Solid State Electron, 1961; 3: 37
2 Pfann W G. Trans AIME, 1952; 194: 747
3 #12
4 Wilke C R, Lee C Y. Ind Eng Chem, 1955; 47: 1253
5 Treybal R E, Mass-Transfer Operations, 2nd ed, New York: McGraw-Hill, 1968: 24-28
6 Brandes E A. In: Brandos E A ed., Smithells Metals Reference Book, 6th ed, London: Butterworths, 1983: 8-54
7 Coulson J M et al. Chemical Engineering, Vol. 1, 3rd ed., Oxford: Pergamon, 1977: 277
8 Hirschfelder J O, Bird R B, Spotz E L. J Chem Phys, 1948; 16: 968
No related articles found!