| DISTRIBUTION OF Mg IN A Ni-BASE SUPERALLOY |
| MA Peili; ZHUANG Jingyun; YANG Jinyan; GAO Liang (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 25 October; 1985; revised manuscript 16 June; 1986) |
|
Cite this article:
MA Peili; ZHUANG Jingyun; YANG Jinyan; GAO Liang (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 25 October; 1985; revised manuscript 16 June; 1986). DISTRIBUTION OF Mg IN A Ni-BASE SUPERALLOY. Acta Metall Sin, 1987, 23(3): 195-199.
|
|
|
Abstract The distribution of Mg in a Ni-base superalloy was observed to be not only enriched along the grain boundaries, but also entered into the secondary carbides of grain boundaries and γ'-phase, either along grain boundary or in the grains.
|
|
Received: 18 March 1987
|
1 #12 2 #12 3 可大年,仲增墉。金属学报,1983;19:A377-A384 4 Debarbodillo J J,郭文通译.高温合金:冶金学和生产,上海科学技术出版社,1980:58-67 5 Yamaguchi S, Kobayashi H, Matsumiya T, Hayami S. Met Technol, 1979; 6: 170-175 6 Guttmann M, Quantin B, Dumoulin Ph. Met Sci, 1983; 17(3) : 123-140 7 染野檀,安盛岩雄编,郑伟谋译。表面分析,科学出版社,1980:208 8 可大年,仲增墉.钢铁研究总院学报,1983;3(1) :73-80 9 藤田利夫,柴田诰司。日本金属学会会報,1977;16:231-238 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|