AN OBSERVATION OF CRYSTALLINE STEPS IN CAST IRON
by ZHAO Jian (Central Iron and Steer Research Institute; Ministry of Metallurgical Industry; Beijing)
Cite this article: 

by ZHAO Jian (Central Iron and Steer Research Institute; Ministry of Metallurgical Industry; Beijing). AN OBSERVATION OF CRYSTALLINE STEPS IN CAST IRON. Acta Metall Sin, 1986, 22(6): 84-150.

Download:  PDF(1367KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The pattern of crystalline steps on the fracture surface of cast iron were observed by SEM. It was found that the dendrites of cast iron grow not only along <100> directions but also along <110> directions. All the crystalline steps belong to {100} and {110} planes.
Received:  18 June 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I6/84

1 Fellow, J.A., Metals Handbook, Vol. 9, 8th, 1974, ASM Metals, Park, Ohio, p. 44073.
2 周敬;常昕;郭可信,金属学报,14(1978) ,246.
3 Pittinato, G.F.; Kerlins. V.; Phillips, A.; Russo, M.A., SEM/TEM Fractography Handbook, Metals and Ceramics Information Center, Columbus, 1975, p. 56.
4 Engel-Klingele, Rasterele Ktrnenmikroskopische Untersuchungen von Metallschaeden, Gerling Institut fuer Schadenforschung und Schadenverhuetung Gmbh, Koln, 1974, p. 114.
5 1972, p. 222.
6 陈廉;徐永波;尹万全,金属学报,14(1978) ,251.
7 Verhoeven, J.D., Fundamentals of Physical Metallurgy. John Wiley & Sons, New York, 1975, p. 244.X
No related articles found!
No Suggested Reading articles found!