Acta Metall Sin  1986, Vol. 22 Issue (6): 86-88    DOI:
Current Issue | Archive | Adv Search |
INFLUENCE OF P ON FRACTURE MORPHOLOGY OF Cr-Mn-Si STEEL WITH PEARLITE, BAINITE AND MARTENSITE STRUCTURES
by ZHU Xun; LI Lidan (He bei Institute of Mecahnical and Electrical Engineering; Shijiazhuang); WANG Jucai (Taihang Machine Works)
Cite this article: 

by ZHU Xun; LI Lidan (He bei Institute of Mecahnical and Electrical Engineering; Shijiazhuang); WANG Jucai (Taihang Machine Works). INFLUENCE OF P ON FRACTURE MORPHOLOGY OF Cr-Mn-Si STEEL WITH PEARLITE, BAINITE AND MARTENSITE STRUCTURES. Acta Metall Sin, 1986, 22(6): 86-88.

Download:  PDF(1385KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The influence of P on impact toughness test and SEM observation was investigated on the 30CrMnSiA steel with pearlite, bainite and martensite-bainite mixed structures. Results showed that the cleavage element on the fracture surface increases and the impact toughness decreases as the increasing of P content. The intergranular fracture appeared till P up to 0.020%. An impact toughness sequence of various structures in the steel influenced by P may be arranged as: martensite+bainite>bainite>pearlite.
Received:  18 June 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I6/86

1 Jokl, M.L.; Kameda, Jun.; McMahon, C.J., Jr.; Vitek, V., Met. Sci., 14 (1980) , 375.
2 Zia-Ebrahimi. F.; Krauss, G.o Metall. Trans., 14A (1983) , 1109.
3 朱勋;李立丹;王士本;王聚才,金属学报,21(1985) ,A 139.
4 Mulford, R.A.; McMahono C.J., Jr.; Pope, D.P.; Feng, H.C., Metall. Trans., 7A (1976) , 1183.
No related articles found!
No Suggested Reading articles found!