ON THE ORDERED NIOBIUM CARBIDE IN MICROALLOY STEELS
by YONG Qilong; ZHENG Lu; SUN Zhenbao (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing)
Cite this article: 

by YONG Qilong; ZHENG Lu; SUN Zhenbao (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing). ON THE ORDERED NIOBIUM CARBIDE IN MICROALLOY STEELS. Acta Metall Sin, 1986, 22(6): 81-83.

Download:  PDF(467KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The precipitated niobium carbide is revealed to be ordered in ferrite in 3 different microalloyed steels containing Nb about 0.08—0.24%. This ordered niobium carbide may be formulated as Nb_8C_7~′(NbC_(0.875)~′) which is formed by ordered omission of its C atoms. With the reciprocal lattice indexes or orientation relationship of transformation matrix between the ordered niobium carbide and α-Fe, the composite electron diffraction patterns can be conveniently indexed.
Received:  18 June 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I6/81

1 De Novion, C.H.; Lorenzelli, R.; Costa, P., C. R. Hebd. Seances Acad. Sci., 263 (1966) , 775.
2 Venables, J.D.; Kahn. D.; Lye, R.G., Philos. Mag., 18 (1968) , 177.
3 Froidevaux, C.; Rossier, D., J. Phys. Chem. Solids, 28(1967) , 1197.
4 Kordes, D., Phys. Status Solidi, 26 (1968) , k103.
5 Billingham, J.; Lewis, M. H. 7th Int. Congress for EM, Grenoble 1970, p. 477.
6 Hollox, G.E.; Edington, J. W.; Scarlin, R. B., J. Iron Steel Inst., 209 (1971) , 839.
7 Scarlin, R.B.; Edington, J. W., J. Mater. Sci., 9 (1974) , 1590.
8 Dunlop, G.L.; Porter, D.A., Scand. J. Met., 16 (1977) , 19.
9 董企铭,硕士论文,冶金部钢铁研究总院,1981.
10 雍岐龙,郑鲁,金属学报,20(1984) ,19.
11 Nordberg, H.; Aronsson, B., J. Iron Steel Inst., 206 (1968) , 1263.
12 Nagakura, S.; Oketani, S., Trans. Iron Steel Inst. Jpn., 8 (1968) , 265
No related articles found!
No Suggested Reading articles found!