Please wait a minute...
Acta Metall Sin  1986, Vol. 22 Issue (6): 135-138    DOI:
Current Issue | Archive | Adv Search |
THERMAL EXPANSION OF PdSi-BASE AMORPHOUS METALS AND THEIR VOLUME EFFECT ON TRANSFORMATION
by ZHENG Fuqian; HU Jiansong (Institute of Precious Metals Reseaerch; Kunming)
Cite this article: 

by ZHENG Fuqian; HU Jiansong (Institute of Precious Metals Reseaerch; Kunming). THERMAL EXPANSION OF PdSi-BASE AMORPHOUS METALS AND THEIR VOLUME EFFECT ON TRANSFORMATION. Acta Metall Sin, 1986, 22(6): 135-138.

Download:  PDF(308KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The volume effect of 6 PdSi-base amorphous alloys on heating has been measured by a tension method. The fractional free volume of 3 ternary alloys at the glass transition temperature is calculated to be 0.02—0.03 which is approaching the value 0.025 of ordinary amorphous materials. The relationship between free volume increment of 6 materials in equilibrium state and relative viscosity is consistent with the viscous flow free volume model.
Received:  18 June 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I6/135

1 Chen, H.S.,; Krause, J.T.; Sigety, F. A., J. Non-Cryst. Solids, 13 (1973/74) , 321.
2 Shelby, J.E., J. Non-Cryst. Solids, 34 (1979) , 111.
3 Brooks, H. A., J. Appl. Phys., 49 (1978) , 213.
4 Tan Qing-Lin (谭庆麟); Liu Xiong (刘雄); Zheng Fuqian (郑福前); Gao Yiqun (高逸群), Thermal Analysis, Vol. 1, Proc. of the 7th Int. Conf. on Thermal Analysis, Ed. Miller, B., Wiley, Heyden, 1982, p. 406.
5 高逸群;郑福前;刘雄;廖宗尧,金属学报,18 (1982) ,696。
6 Williams, M.L.; Landel, R.F.; Ferry, J.D., J. Am. Chem. Soc., 77 (1955) , 3701.
7 Ramachandrarao, P.; Cantor, B.; Cahn R.W.; J. Mater, Sci., 12 (1977) , 2488.
8 郑福前;廖宗尧;胡健松,金属学报,22 (1986) ,B15
No related articles found!