Abstract A new method for the simultaneous determination of the Ce subgroup and Y in Ni-base alloy or steel was developed. The trouble to analysis from the mutual overlap on the spectra resulted by the complexes of Ce sub-group and Y with chlorophosphonazo-P-NO_2 in HClO_4 has been relieved by complete separation using first derivative spectrophotometry. The interference of foreign ions can be eliminated by masking with VC, Zn-EDTA and NH_4F. The method has been applied to Ni-base alloy or steel containing 0.05—0.4% Ce sub-group and Y with a relative error ±8%.
|
|
Received: 18 June 1986
|
1 潘教麦,化学试剂,(1981) ,№ 4,48。 2 孙慧芳;潘教麦;黄留庆,理化检验,19 (1983) ,№ 1,11。 3 马玉珊,冶金分析,待发表。 4 孙若诚,稀有金属,8 (1984) ,№ 1,56。 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|