THEORETICAL ESTIMATION OF FATIGUE LIFE OF DRILL ROD
SONG Shouzhi; XU Xiaohe (Northeast Institute of Technology; Shenyang)
Cite this article: 

SONG Shouzhi; XU Xiaohe (Northeast Institute of Technology; Shenyang). THEORETICAL ESTIMATION OF FATIGUE LIFE OF DRILL ROD. Acta Metall Sin, 1986, 22(5): 134-136.

Download:  PDF(729KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An approach was made theoretically to the load spectrum for the drill rod under striking. A source programme has been written to computer the drilling load oscillogram of a striking-penetrating system. The theoretical estimation of the fatigue life of the drill rod is carried out bY analyzing the rule and constitution of the load spectrum and its influence on the surplus life of drill rod.
Received:  18 May 1986     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1986/V22/I5/134

1 Newland, D.E., An Introduction to Random Vibrations and Spectral Analysis, Longman Group Ltd., Edinburgh, 1975, p. 42.
2 徐小荷,岩石力学与工程学报,3(1984) ,№1,75.
3 长沙矿冶研究院;贵阳钎钢研究所,矿冶工程,5(1985) ,№1,3.
4 徐濒,疲劳强度设计,机械工业出版社,1981,P.210.
5 宋守志;徐小荷;李润隆,钢铁,21(1986) ,№3,30.?
No related articles found!
No Suggested Reading articles found!