THE THERMAL STABILITY OF PdTa_1 Si_(16.5) ALLOY OF DIFFERENT GLASSY STATES
by NING Yuantao; ZHENG Yun(Institute of Precious Metals; Ministry of Metallurgical Industry; Kunming)(Manuscript received 26 April; 1983; revised manuscript 27 July; 1983)
Cite this article: 

by NING Yuantao; ZHENG Yun(Institute of Precious Metals; Ministry of Metallurgical Industry; Kunming)(Manuscript received 26 April; 1983; revised manuscript 27 July; 1983). THE THERMAL STABILITY OF PdTa_1 Si_(16.5) ALLOY OF DIFFERENT GLASSY STATES. Acta Metall Sin, 1984, 20(2): 154-158.

Download:  PDF(356KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The thermal stability and the crystallization of PdTa_1Si_(16.5) alloy of different glassy states have been studied by means of the differential scanning calorimeter (DSC). The behaviour of glass transformation and crystallization as well as the thermal stability in both states as-quenched and as-annealed are varied with the non-crystalline alloys of different glassy state owing to change of the quenching rates.
Received:  18 February 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I2/154

1 Gao Yi-Qun(高逸群); Zheng Fu-Qian(关福前); Liu Xiong(刘雄);Ning Yuan-Tao(宁远涛), Proc. 4th Int. Conf. on Rapidly Quenched Metals(Sendai, 1981) , Eds. Masumoto, T.; Suzuki, K., JIM, 1982, Vol. 1, p. 727.
2 Chen, H. S., Appl. Phys. Lett., 29(1976) , 12.
3 Chen, H. S., Rep. Prog. Phys., 43(1980) , 353.
4 Freed, R. L.; Vander Sande, J. B., Acta Metall., 28(1980) , 103.
No related articles found!
No Suggested Reading articles found!