MOSSBAUER STUDY OF Fe-Ni INVAR ALLOYS MINGLED WITH Pr
by JIN Mingzhi (Jilin University; Chanschun); YU Enhua; SUN Shaozhou(Northeast Institute of Technology; Shenyang)(Manuscript received 28 June; 1982; revised manuscript 18 August; 1983)
Cite this article: 

by JIN Mingzhi (Jilin University; Chanschun); YU Enhua; SUN Shaozhou(Northeast Institute of Technology; Shenyang)(Manuscript received 28 June; 1982; revised manuscript 18 August; 1983). MOSSBAUER STUDY OF Fe-Ni INVAR ALLOYS MINGLED WITH Pr. Acta Metall Sin, 1984, 20(2): 159-165.

Download:  PDF(486KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The magnetic structural properties and the effect of trace in Pr mingled upon the structure and properties of the Fe-Ni Invar alloy have been analyzed by M(?)ssbauer spectrum. It was resulted that the co-existence of Fe ions with ferromagnetism and anti-ferromagnetism seems to the nature of the alloy having the Invar charater. And the Invar character of the Fe-Ni Invar alloy maintains even mingled with a trace of Pr, yet its macro-magnetism is reduced.
Received:  18 February 1984     

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I2/159

1 Nakamura, Y., IEEE Trans. on Magnetics., 12(1976) 278.
2 金明芝;孙绍周;于恩华,东北工学院学报,3(1983) ,№36,35.
3 Bhide, V. G., Mossbauer Effect and Its Applications, New Delhi, 1973, p. 196.
4 Teble, R. S.; Graik, D. J., Magnetic Materials, Wiley, London, 1969, p. 51 Table 2. 16.
5 Abrahams, S. C.; Guttman, L.; Kaspet, J. S., Phys. Rev., 127(1962) , 2052.
6 Menshikov, A. Z., J. Magn. Magn. Mater., 10(1979) , 205.
7 Komura, S.; Takeda, T. J., ibid., 10 (1979) , 191.
8 #12
9 #12
10 Hausch, G.; Z. Metallk., 63(1972) , 547.
11 Gignoux, D.; Givord, D.; Givord, F.; Lemaire, R., J. Magn. Magn. Mater., 10(1979) , 288.
12 Givord, D.; Lemaire, R.; James, W. J.; Moreau, J. M.; Shah, J. S., IEEE Trans. Magn., 7 (1971) , 657.
13 Gubbens, P. C. M.; Van Loef, J. J.; Buschow, K. H. J., J. Phys., (Paris), Colloq. C6(1974) , 617.
14 Elemans, J B. A. A.; Gubbens, P. C. M.; Buschow, K. H. J., J. Less-Common Met., 44(1976) , 51.
15 苟清泉,固体物理简明教程,人民教育出版社,1979,p.143.
No related articles found!
No Suggested Reading articles found!