MAXIMUM SOLUBILITY VARIATION OF Si, Ge, Sn OR Pb IN Ti
by WANG Kongtan (Luoyang Institute of Ship Material Research)
Cite this article: 

by WANG Kongtan (Luoyang Institute of Ship Material Research). MAXIMUM SOLUBILITY VARIATION OF Si, Ge, Sn OR Pb IN Ti. Acta Metall Sin, 1983, 19(3): 112-117.

Download:  PDF(456KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The variation of maximum solubilities, C_α and C_β, of the element of group IVA such as Si, Ge, Sn or Pb in α-and β-Ti have been discussed by statistical analysis, It is shown that the variations of C_α and C_β are controlled simultaneously by the metallicity of the element and by the difference between the atomic radii of Ti and the element of group IVA. The effect of metallicity on C_β is more predominate than that on C_α, while the effect of difference between atomic radii on C_β is less than that on C_α. This variation seems to be of common significance.
Received:  18 March 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I3/112

1 The Science Technology and Application of Titanium, Eds. Jaffee, R. I.; Promisel, N. E., Pergamon Press, London, 1970, p. 407.
2 陈念贻,键参数函数及其应用,科学出版社,1976,pp.15-17,107-108.
3 葛志明,钛的二元系相图,国防工业出版社,1978,pp.29-30,65-68.
4 Zwicker, U., Titan und Titanlegierugen, Springer-Verlag, Berlin, 1974,p. 154.
No related articles found!
No Suggested Reading articles found!