Abstract The variation of maximum solubility C_α of S, Se or Te in α-Ti has been calculated by solving the proposed equation. It was shown that the equation is also available to Po, its C_α =0.21 at.-% and the effective electric charge z~*=5.26. The maximum solubility C_β of S, Se, Te or Po in β-Ti was estimated to be 0.13, 0.24, 0.29 or 0.32 at.-% respectively by the correlation between C_β and C_α. Thevariations of C_α and C_β of the elements of group VIA are controlled by nonmetallicity and the difference between the radii of atoms of these elements and Ti, and mainly by their non-metallicity. C_α and C_β have good linear relationships with the difference between electronegativity, the ratio of electric charge and radius of Ti or these elements, the ratio of electric charge and radius of these elements and the difference between atomic radii of Ti and these elements. C_α and C_β decrease linearly with the increase of these parameters.
|
|
Received: 18 March 1983
|
1 #12 2 #12 3 The Science Technology and Application of Titanium, Eds. Jaffee, R. I.; Promisel, N. E., Pergamon Press. London, 1970, p. 407. 4 陈念贻,键参数函数及其应用,科学出版社,1976. 5 王孔探,金属学报,19(1983) ,B112. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|