DETERMINATION OF LATTICE STABILITY PARAMETERS AND THEIR APPLICATION
by WANG Mingxian (Institute of Metal Research; Academia Sinica; Shenyang)
Cite this article: 

by WANG Mingxian (Institute of Metal Research; Academia Sinica; Shenyang). DETERMINATION OF LATTICE STABILITY PARAMETERS AND THEIR APPLICATION. Acta Metall Sin, 1983, 19(3): 106-111.

Download:  PDF(460KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A method is proposed for ascertaining the lattice stability parameters, offering an example of 5 binary phase regions in Cu-Ag and Pb-T1 systems, on the basis of a few thermodynamical data and the state function properties. The calculated binary phase boundaries by using these parameters are in good agreement with the experimental results. Thus, the phase equilibrium among the solid solutions with fee structure in Cu-Ag system has been discussed.
Received:  18 March 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I3/106

1 Kaufman, L., Metallurgical Chemistry, NPL, England, 1972, p. 375.
2 Ansara, I., Int. Met. Rev., 1 (1979) , 25.
3 Hillert, M., Calculation of Phase Diagrams and Thermochemistry of Alloy Phases, The Metall. Soc. of AIME, 1979, p. 3.
4 Hultgren, R., Selected Values of the Thermodynamic Propertes of Binary Alloys, ASM, 1973, p. 1277.
5 Hultgren, R. ibid., p. 1280.
6 Hultgren, R., Selected Values of Thermodynamic Properties of the Elements, ASM, 1973, p. 526.
7 Hultgren, R., ibid., p. 382.
8 王明贤,雷琼芝,金属学报,18(1982) ,627.
9 Hultgren, R., Selected Values of the Thermodynamic Properties of Binary Alloys, ASM,1973, p. 45.
10 Hultgren, R., ibid., p.47.
11 Michaels, K. F.; Lange, W. F.; Bradley, J. R.; Aaronson, H. I., Metall. Trans., 6A (1975) , 1843.
12 徐祖耀,金属学原理,上海科学技术出版社,1963. p.217.
13 徐祖耀,金属材料热力学,科学出版社 1981. p.210,276.
14 Jantzen, C. M. F.; Herman, H., Phase Diagrams, Materials Science and Technology, Ed. Alper, A, M., Vol. 5, 1978, p. 155.
No related articles found!
No Suggested Reading articles found!