A STUDY OF THE TEXTURES OF ARMCO IRON BY MAGNETIC TORQUE METHOD
TAI LI-CHI(L.C.TAI)AND WANG CHIEN-KANG Iron and Steel Research Institute
Cite this article: 

TAI LI-CHI(L.C.TAI)AND WANG CHIEN-KANG Iron and Steel Research Institute. A STUDY OF THE TEXTURES OF ARMCO IRON BY MAGNETIC TORQUE METHOD. Acta Metall Sin, 1958, 3(1): 47-54.

Download:  PDF(522KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The rolling and recrystallization textures of armco iron are measured by magnetictorque method.Samples after hot-rolling are then cold rolled in three different ways;i.e.,thepercentages of the cold reduction are(i)73,(ii)65 and(iii)22.The class Ⅰ andclass Ⅲ material are annealed for one hour either at 700° or 850℃,and then givena second cold roll,the reduction of class Ⅰ material being this time 65 per cent andclass Ⅲ material being 55 per cent.All these samples in these three categories aregiven a final anneal at 870℃ in hydrogen for ten hours.The textures of the samples through one cycle of cold rolling are determined as(100)[011]and(112)[110].The textures of the material through two cycles ofcold rolling,with an intermediate anneal,are mainly(112)[110].The final annealedsamples with the possible exception of the class Ⅲ are estimated as having textures(110)[001]and(110)[001]+(100)[001].
Received:  18 January 1958     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1958/V3/I1/47

[1] Wassermann,G.,Texturen metallischer Werkstoffe(1939) .
[2] Goss,N.P.,Trans.A.S.S.T.,16(1929) ,405.
[3] Stanley,J.K.,Trans.A.I.M.E.,158(1944) ,354.
[4] #12
[5] Kurdjumov,G.u Sachs,G.,ZS.für Physik,62(1930) ,592.
[6] Haeβner,F.u Weik,H.,Archiv des Eisenhüttenw.,27,Heft 3(1956) ,153.
[7] 戴礼智,张信钰,国产纯铁轧[制与再结晶织构,物理学报,第14卷,第1期.
[8] Bozorth,R.M.,Ferromagnetism(1951) ,ch.XII.q
No related articles found!
No Suggested Reading articles found!