Please wait a minute...
Acta Metall Sin  1958, Vol. 3 Issue (1): 55-61    DOI:
Current Issue | Archive | Adv Search |
FORMATION OF ANNEALING TWINS IN α-IRON
CHUANG YU-CHIH AND WU CHEUNG-HUNG Institute of Metal Research;Academia Sinica
Cite this article: 

CHUANG YU-CHIH AND WU CHEUNG-HUNG Institute of Metal Research;Academia Sinica. FORMATION OF ANNEALING TWINS IN α-IRON. Acta Metall Sin, 1958, 3(1): 55-61.

Download:  PDF(2397KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Twin formation associated with grain boundary migration in recrystallized armcoiron has been studied by the method of vacuum etching.No noticable substructureswere observed after recrystallization at 750℃ for 5 hours.However,after reheatingfor a short time at 770℃,fine substructures appeared in most of the ferrite grains.During prolonged heating the substructure-free grains gradually grew at the expense ofthose possessing substructures.When the reheating temperature is raised close to theA_3 temperature,grain boundary migration is markedly accelerated.Two types of twins were observed during grain growth.One of them,probablyidentical in nature with ordinary annealing twins,has its non-coherent twin boundaryalways attached to the old grain boundary.Depending on the manner of migrationof the grain boundary and the non-coherent twin boundary,such type of twins maygrow,retreat,or even disappear.The other type of twins has a characteristic wedge-shaped twin boundary which is quite stable,and little change has been observed afterprolonged heating.
Received:  18 January 1958     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1958/V3/I1/55

[1] Tamura,S.J.,Journal of Iron & Steel Inst.,115(1927) ,747.
[2] O'Neill,H.,Journal of Iron & Steel Inst,117(1928) ,689.
[3] Greninger,A.B.,Trans.Amer.Inst.Mining & Metallurgical Engineers,120(1936) ,293.
[4] Barrett,C.S.,Trans.Amer.Inst.Mining & Metallurgical Engineers,Discussions,173(1940) ,190.
[5] #12
[6] Shuttleworth,R.,Metallurgia,38(1948) ,125.
[7] Burke,J.E.,Trans.Amer.Inst.Mining & Metallurgical Engineers,188(1950) ,1324.
[8] Burke,J.E.and Turnbull,D.,Progress in Metal Physics,vol.3(1952) ,220.
[9] #12
[10] Hall,E.O.,Twinning & Diffusionless Transformations in Metals(Butterworths Scientific Publications,London),1954.
[11] Dunn,C.G.,Daniels,F.W.and Bolton,M.J.,Trans.Amer.Inst.Mining & Metallurgical Engineers,188(1950) ,368.
[12] Ellis,W.C.and.Treuting,R.G.,Trans.Amer.Inst.Mining & Metallurgical Engineers,191(1951) ,53.
[13] Fullman,R.L.and Fisher,J.C,Journal of Applied Physics,22(1951) ,1350.
No related articles found!
No Suggested Reading articles found!