Acta Metall Sin  2013, Vol. 49 Issue (10): 1153-1159    DOI: 10.3724/SP.J.1037.2013.00159
Current Issue | Archive | Adv Search |
HYDROGEN INDUCED DELAYED FRACTURE BEHAVIOR OF A LOW-CARBON Mn-B TYPE ULTRA-HIGH STRENGTH STEEL SHEET AFTER HOT STAMPING
ZHANG Yongjian, HUI Weijun, DONG Han
National Engineering Research Center of Advanced Steel Technology, Central Iron and Steel Research Institute, Beijing 100081
Cite this article: 

ZHANG Yongjian, HUI Weijun, DONG Han. HYDROGEN INDUCED DELAYED FRACTURE BEHAVIOR OF A LOW-CARBON Mn-B TYPE ULTRA-HIGH STRENGTH STEEL SHEET AFTER HOT STAMPING. Acta Metall Sin, 2013, 49(10): 1153-1159.

Download:  PDF(2212KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

In consideration of the light weight and the impact safety of cars, in recent years, hot stamping has been increasingly applied to the manufacture of car parts, which has driven forward the increasing use of ultra-high strength steel sheet in the automobile industry. However, when the tensile strength of steel is more than about 1200 MPa, the steel sheet is very susceptible to hydrogen induced delayed fracture. Up to now, some research has been carried out on delayed fracture behavior of both high strength and ultra-high strength steel sheet. However, the delayed fracture behavior of a low-carbon Mn-B type steel sheet widely used for hot stamping has not been paid enough attention and fully studied. There are also a scarcity of reports on hydrogen induced delayed fracture behavior of this steel sheet after hot stamping. With the development of the hot stamping, the evaluation of delayed fracture behavior of ultra-high strength steel sheet for hot stamping, especially the delayed fracture behavior of steel sheet after hot stamping has become very urgent. For these reasons, hydrogen induced delayed fracture behavior of a low-carbon Mn-B type ultra-high strength hot stamping steel sheet at both the hot stamped status and the common quenched and tempered status was studied by means of constant load delayed fracture test and hydrogen thermal desorption spectrometry (TDS) analysis. The results show that both the critical delayed fracture stress σc and delayed fracture life of the steel sheet after hot stamping process are higher than as-quenched sample, and it even matches the level of the quenched +100℃ tempered sample. Moreover, the σc of the steel sheet could be further improved by tempering at 200℃. The delayed fracture surface observed by SEM shows that, under the effect of applied stress and corrosive liquid, the fracture characteristic of the hot stamped sample at crack initiation area changes from brittle intergranular failure in the as-quenched condition to ductile transgranular failure in the hot stamped condition. Furthermore, the TDS result shows that the hydrogen content of steel sheet significantly increases when the steel sheet was applied at critical stress for 100 h in the corrosive liquid. In addition, the hot stamping steel sheet can withstand more hydrogen content than as-quenched sample and quenched +100℃ tempered sample due to the sufficient self tempering. As a result, the hot stamping sample gets a higher critical delayed fracture stress. Therefore, the steel has good delayed fracture resistance after hot stamping, and the delayed fracture resistance of the steel sheet could be further improved by tempering.

Key words:  low-carbon Mn-B steel      ultra-high strength steel sheet      hot stamping      hydrogen induced delayed fracture      hydrogen thermal desorption spectrometry analysis     
Received:  03 April 2013     

URL: 

https://www.ams.org.cn/EN/10.3724/SP.J.1037.2013.00159     OR     https://www.ams.org.cn/EN/Y2013/V49/I10/1153

[1] Nicolas Y.  Thyssen  Krupp Techforum, 2005; (7): 40

[2] Geiger M, Merklein M, Hoff C.  Adv Mater Res, 2005; 6-8: 795
[3] Altan T.  Stamping J, 2006; (12): 40
[4] Sato M, Utsumi Y, Watanabe K.  Kobelco Technol Rev, 2008; 28: 13
[5] Karbasian H, Tekkaya A E.  J Mater Process Technol, 2010; 210: 2103
[6] Lee S J, Ronevich J A, Krauss G, Matlock D K.  ISIJ Int, 2010; 50: 294
[7] Hein P, Wilsius J.  Steel Res Int, 2008; 79(2): 85
[8] Suehiro M, Maki J, Kusumi K, Ogami M, Miyakoshi T.  Nippon Steel Tech Rep, 2003;(88): 16
[9] Chu W Y.  Hydrogen Damage and Delayed Fracture. Beijing: Metallurgy Industry Press, 2000: 149
(褚武扬. 氢损伤与滞后断裂. 北京: 冶金工业出版社, 2000: 149)
[10] Hui W J, Weng Y Q, Dong H.  High-Strength Fasteners Steels. Beijing: Metallurgy Industry Press, 2009: 32
(惠卫军, 翁宇庆, 董瀚. 高强度紧固件用钢. 北京: 冶金工业出版社, 2009: 32)
[11] Hoji T, Sugimoto K, Mukai Y.  Tetsu Hagane, 2006; 92: 83
(北蓧智彦, 杉本公一, 向井陽一. 鉄と鋼, 2006; 92:83)
[12] Hojo T, Sugimoto K, Mukai Y.  ISIJ Int, 2008; 48: 824
[13] Toji Y, Takagi S, Yoshino M, Hasegawa K, Tanaka Y.  Mater Sci Forum, 2010; 638-642: 3537
[14] Qi J Y, Li Y J, Zhou H J.  Trans Met Heat Treat, 1984; 5(1): 42
(齐靖远, 黎永钧, 周惠久. 金属热处理学报, 1984; 5(1): 42)
[15] Li G F, Dong H, Gao W, Zhao Y J.  J Iron Steel Res, 1996; 8(5): 42
(李桂芬, 董瀚, 高伟, 赵玉君. 钢铁研究学报, 1996; 8(5): 42)
[16] Li G F, Wu R G, Lei T Q.  J Chin Soc Corros Prot, 1991; 11: 27
(李光福, 吴忍田井, 雷廷权. 中国腐蚀与防护学报, 1991; 11: 27)
[17] Chu W Y, Li S Q, Xiao J M, Wang C.  Acta Metall Sin, 1980; 16: 179
(褚武扬, 李世琼, 肖纪美, 王枨. 金属学报, 1980; 16: 179)
[18] Nakatani Y, Higashi T, Yamada K.  Fatigue Fract Eng Mater Struct, 1999; 22: 393
[19] Hui W J, Dong H, Weng Y Q, Wang M Q, Shi J.  Trans Mater Heat Treat, 2006; 27(6): 37
(惠卫军, 董瀚, 翁宇庆, 王毛球, 时捷. 材料热处理学报, 2006; 27(6): 37)
[20] Takahashi T, Yamasaki S.  Kinzoku, 1997; 67: 1011
(高橋稔彦, 山崎眞吾. 金属, 1997; 67: 1011)
[21] Suzuki N, Ishii N, Miyagawa T, Harada H.  Tetsu Hagane, 1993; 79: 227
(鈴木信一, 石井伸幸, 宮川敏夫, 原田宏明. 鉄と鋼, 1993; 79: 227)
[1] ZHU Bin, YANG Lan, LIU Yong, ZHANG Yisheng. Micromechanical Properties of Duplex Microstructure of Martensite/Bainite in Hot Stamping via the Reverse Algorithms in Instrumented Sharp Indentation[J]. 金属学报, 2022, 58(2): 155-164.
[2] YI Hongliang,CHANG Zhiyuan,CAI Helong,DU Pengju,YANG Dapeng. Strength, Ductility and Fracture Strain ofPress-Hardening Steels[J]. 金属学报, 2020, 56(4): 429-443.
[3] JIN Xuejun,GONG Yu,HAN Xianhong,DU Hao,DING Wei,ZHU Bin,ZHANG Yisheng,FENG Yi,MA Mingtu,LIANG Bin,ZHAO Yan,LI Yong,ZHENG Jinghua,SHI Zhusheng. A Review of Current State and Prospect of the Manufacturing and Application of Advanced Hot Stamping Automobile Steels[J]. 金属学报, 2020, 56(4): 411-428.
[4] HUI Yajun, LIU Kun, WU Kemin, LI Qiuhan, NIU Tao, WU Qiaoling. Effect of Coiling Temperature on Microstructure and Mechanical Properties of 500 MPa Grade Hot Stamping Axle Housing Steel[J]. 金属学报, 2020, 56(12): 1605-1616.
[5] Xunhua YUAN, Qifu ZHANG. Microstructure Evolution of Hot-Dip Al-10%Si Coating During the Austenitization of 22MnB5 Hot Stamping Steel[J]. 金属学报, 2017, 53(11): 1495-1503.
[6] CHENG Junye, ZHAO Aimin, CHEN Yinli, DONG Rui, HUANG Yao. EBSD STUDIES OF 30MnB5 HOT STAMPING STEEL TEMPERED AT DIFFERENT TEMPERATURE[J]. 金属学报, 2013, 49(2): 137-145.
[7] WANG Yanfei GONG Jianming JIANG Wenchun JIANG Yong TANG Jianqun . NUMERICAL SIMULATION OF HYDROGEN INDUCED DELAYED FRACTURE OF AISI4135 HIGH STRENGTH STEEL USING COHESIVE ZONE MODELING[J]. 金属学报, 2011, 47(5): 594-600.
[8] GAO Kewei; WANG Yanbin; CHU Wuyang (University of Science and Technology Beijing; Beijing 100083) (Manuscript received 1995-04-11; in revised form 1995-09-11 ). HYDROGEN INDUCED DELAYED FRACTURE OF TiAl ALLOY AT ROOM TEMPERATURE[J]. 金属学报, 1996, 32(1): 29-32.
[9] HU Wei;WANG Yanbin;CHU Wuyang;XIAO Jimei University of Science and Technology Beijing Correspondent associate professor; Deparment of Materials; University of Science and Technology Bejing; Bejing 100083. HYDROGEN EMBRITTLEMENT IN Ni-Fe FCC ALLOYS AND EFFECT OF COMPOSITION[J]. 金属学报, 1992, 28(6): 1-6.
No Suggested Reading articles found!