| 不对称性定量化的三元系热力学模型 |
| 沈剑韵;郝耀武;周传华;凌铃 |
| 北京有色金属研究总院 |
|
| A MODEL WITH QUANTIFIED ASYMMETRY FOR PREDICTING THERMODYNAMIC PROPERTIES OF TERNARY SYSTEM |
| SHEN Jianyun; HAO Yaowu; ZHOU Chuanhua; LING Ling (General Research Institule for Non-Ferrous Metals; Beijing 100088) |
引用本文:
沈剑韵;郝耀武;周传华;凌铃. 不对称性定量化的三元系热力学模型[J]. 金属学报, 1996, 32(9): 943-948.
,
,
,
.
A MODEL WITH QUANTIFIED ASYMMETRY FOR PREDICTING THERMODYNAMIC PROPERTIES OF TERNARY SYSTEM[J]. Acta Metall Sin, 1996, 32(9): 943-948.
| 1KohlerF,Monat.FuerChemie,1960;91:7382MuggianuYM,GambinoM,BrosJP.ChemPhys,1975;22:833ToopGM.TransAIME,1965;233:8504ChouGC.CALPHAD,1994;24:385ChouGC.CALPHAD,1995;25:646QiaoZY,XingXR,ZhengCQ,DuanSZ.JRareEarths,1991;9:1817周传华.北京有色金属研究总院博士学位论文,19958LukasHL,HeingET,ZimmermannB.CALPHAD,1977;1:2259SaboungiML,LinPL,CerisierP,PeltonAD.MetallTrans,1980;11B:493 |
|