机械合金化形成的Fe-Cu纳米晶过饱和固溶体的硬化及软化 |
李伯林;朱敏;李隆;罗堪昌;李祖鑫 |
华南理工大学;广州;510641;华南理工大学;广州;510641;华南理工大学;广州;510641;华南理工大学;广州;510641;华南理工大学;广州;510641 |
|
HARDENNING AND SOFTENNING EFFECTS OF Fe-Cu NANOCRYSTALLINE SUPERSATURATED SOLID SOLUTION FORMED BY MECHANICAL ALLOYING |
LI Bolin;ZHU Min; LI Long; LUO Kanchang;LI Zuxin (South China University of Technology; Guangzhou 510641)(Manuscript received 1996-03-19; in revised form 1996-07-15) |
引用本文:
李伯林;朱敏;李隆;罗堪昌;李祖鑫. 机械合金化形成的Fe-Cu纳米晶过饱和固溶体的硬化及软化[J]. 金属学报, 1997, 33(4): 420-426.
,
,
,
,
.
HARDENNING AND SOFTENNING EFFECTS OF Fe-Cu NANOCRYSTALLINE SUPERSATURATED SOLID SOLUTION FORMED BY MECHANICAL ALLOYING[J]. Acta Metall Sin, 1997, 33(4): 420-426.
1 Nieman G W,Weertman J R,Siegel R W.J Mater Res, 1991;6:1012 2 Koch C C, Cho Y S.Nanostruct Mater,1992; 1: 207 3 Lu K,Wei W D,Wang J T.Scr Metall Mater,1990;24:2319 4 Christman T,Jain M.Scr Metall Mater,1991;25:767 5 Nieh T G,Wadseworth.Scr Metall Metaer,1991;25:955 6 Fecht H J.In:Hadjipanayis G C,Siegel R W eds,Nanophase Materials, Klewer Academic publisher,1994: 125 7 Lu K,Sui M L.Scr Metall Mater,1993;28:1465 8 Palumbo G,Thorpe S J,Aust K T.Scr Metall Mater,1990;24:1347 9 Zhu M,Fecht H J.Nanostruct Mater,1995;6:921 10 Uenishi K Kobayashi K F,Nasu S,Hatano H,Ishihara K N,Shingu P H.Z Metallk,1992;83:132 11 Eckert J,Holzer J C,Krill C E, Johnson W L.J Appl Phys,1993;73:2794 12 Yavari A R,Desere P J,Menameur T,Phys Rev Lett,1992;68:2235 13 Ma E, Atzmon M,Pinkerton P E,J Appl Phys,1993;74:955 14 Miedema A R, Broeder F J A. Z Metallk,1979;70:14 |
|