| 以连续铸造方法制备梯度材料的实验研究 |
| 张卫文;邹敢峰;邓长宁;魏兴钊;许麟康;郁鸽 |
| 华南理工大学机电工程系;广州;510641;华南理工大学机电工程系;广州;510641;广州永大机械公司;广州;511443;华南理工大学机电工程系;广州;510641;华南理工大学机电工程系;广州;510641;华南理工大学机电工程系;广州;510641 |
|
| INVESTIGATION OF PRODUCTION OF GRADIENT MATERIAL BY CONTINUOUS CASTING |
| ZHANG Weiwen; ZOU Ganfeng; DENG Changning; WEI Xinzhao; XU Linkang;YU Ge)( Department Mechano-Electronic Engineering ; South China University of Technology; Guangzhou 510641)(Guangzhou Yongda Machninery Company; Guangzhou 511443)Correspondent: YU Ge; professor Tel: (020)87114547; E-mail: metrlab scut edu cn |
引用本文:
张卫文;邹敢峰;邓长宁;魏兴钊;许麟康;郁鸽. 以连续铸造方法制备梯度材料的实验研究[J]. 金属学报, 1998, 34(6): 609-614.
,
,
,
,
,
.
INVESTIGATION OF PRODUCTION OF GRADIENT MATERIAL BY CONTINUOUS CASTING[J]. Acta Metall Sin, 1998, 34(6): 609-614.
1 Cahn R W Haasen P.Physical Metallurgy ,Amsterdam :North -Holland Physics Publishing ,1983: Chspter 2, 4; 5, 10B and 19 to 22 2 Yu G. Deutsches Patentamt, DE4108203 A1, 1991 3 Nino M,Hirai T, Watanabe R. J Jpn Compos Soc, 1987; 13(6): 257 4 Sasaki M, Hirai T J Ceram Soc Jpn, 1991; 99(10): 1002 5 Fady M N, Brian G T, Donald E H. Metall Trans, 1995; 26: 749V |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|