| 纯铜双晶体拉伸变形的介观力学分析 |
| 邹风雷 高克玮 朱其芳 谢建新 |
| 北京科技大学材料学院 |
|
| The mesomechanical analysis of the deformation of copper with continuous columnar crystals |
| ZOU Fenglei; GAO Kewei; ZHU Qifang; XIEJianxin |
引用本文:
邹风雷; 高克玮; 朱其芳; 谢建新 . 纯铜双晶体拉伸变形的介观力学分析[J]. 金属学报, 2008, 44(3): 297-301 .
,
,
,
.
The mesomechanical analysis of the deformation of copper with continuous columnar crystals[J]. Acta Metall Sin, 2008, 44(3): 297-301 .
[1]Zhang H,Xie J X,Wang Z D,Wang H.Mater Mech,2004; 28(2):31 (张鸿,谢建新,王自东,王浩.机械工程材料,2004;28(2):31) [2]Li B,Wang X,Guo J C,Fan X H,Yan W.J Xi'an Inst Technol,2005;25:579 (李炳,王鑫,郭俊仓,范新会,严文.西安工业学院学报,2005;25:579) [3]Wu T K,Liu W.J Tsinghua Univ (Nat Sci),2005;45: 792 (吴廷坤,刘伟.清华大学学报(自然科学版),2005;45:792) [4]Huang X X,Cai D Y,Liu Q,Yao M.Chin J Nonferrous Met,2001;11:110 (黄晓旭,蔡大勇,刘庆,姚枚.中国有色金属学报,2001;11:110) [5]Li H Y,Yah W,Chen J,Fan X H,Wang X Y.J Xi'an Inst Technol,2006;26:64 (李红英,严文,陈建,范新会,王雪艳.西安工业学院学报,2006;26:64) [6]uang X.Scr Mater,1998;38:1697 [7]Wang Z G,Zhang Z F,Li X.W,Jia W P,Li S X.Mater Sci Eng,2001;A319:63 [8]Li X W,Wang Z G,Li S X.Chin J Mater Res,2000;12: 36 (李小武,王中光,李守新,材料研究学报,2000;12:36) [9]Makarov P V.Theor Appl Fract Mech,2000;33:23 [10]Panin V,Kolubaev A,Tarasov S,Popov V.Wear,2002; 249:860 [11]Miravete A,Bielsa J M,Chiminelli A,Cuartero J,Serrano S,Tolosana N.Compos Sci Technol,2006;66:2954 [12]LI Y,Li S X,Li G Y.Acta Metall Sin,2002:38:819 (李勇,李守新,李广义.金属学报,2002;38:819) [13]Yang J X.Fundamental of Metalline Plastic Deformation. Beijng:Metallurgical Industry Press,1988:179 (杨觉先.金属塑性变形物理基础.北京:冶金工业出版社,1988:179) [14]Huang X X,Cai D Y,Yao M,Liu Q,Hansen N.Chin J Nonferrous Met,2001;11:31 (黄晓旭,蔡大勇,姚枚,刘庆,Hansen N.中国有色金属学报,2001;11:31) [15]Chen M A,Li H Z,Li X Q,Liu C M.Mater Sci Eng, 2007;A452:454 [16]Xiao J M,Zhu F W.Study of Material Energy.Shanghai: Shanghai Science & Technology Press,1999:336,400 (肖纪美、朱逢吾.材料能量学.上海:上海科学技术出版社,1999:336,400) [17]Zheng Z Q.Fundamental of Material Sciences.Changsha: Zhongnan University Press,2005:353 (郑子樵.材料科学基础.长沙:中南大学出版社,2005:353) [18]Morinage T,Translated by Jin X Z.Copper and Copper Alloy.Beijing:National Defence Industry Press,1963 (森永卓一著,金宪真译.铜及铜合金.北京:国防工业出版社,1963:77) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|