| 连铸圆坯结晶器的热流计算与讨论 |
| 郭亮亮;姚曼;尹合壁;王旭东;方大成;刘晓;于艳 |
| 大连理工大学材料科学与工程学院 |
|
| CALCULATION AND DISCUSSION ON THE HEAT FLUX IN MOULD OF CONTINUOUS CASTING ROUND BILLET |
| GUO Liangliang; YAO Man; YIN Hebi; WANG Xudong; FANG Dacheng;LIU Xiao; YU Yan |
| 大连理工大学材料科学与工程学院 |
引用本文:
郭亮亮; 姚曼; 尹合壁; 王旭东; 方大成; 刘晓 ; 于艳 . 连铸圆坯结晶器的热流计算与讨论[J]. 金属学报, 2006, 42(9): 983-988 .
,
,
,
,
,
,
.
CALCULATION AND DISCUSSION ON THE HEAT FLUX IN MOULD OF CONTINUOUS CASTING ROUND BILLET[J]. Acta Metall Sin, 2006, 42(9): 983-988 .
[1]Alvarez de Toledo G,Ciriza J,Laraudogoitia J J.Ironmaking Steelmaking,2003;30:360 [2]Yao M,Yin H B.Ironmaking Steelmaking,2005;32:359 [3]Billany T J H,Normanton A S,Mills K C.Ironmaking Steelmaking,1991;18:403 [4]Irving W R,Perkins A.Ironmaking Steelmaking,1977;4:292 [5]Ikeda M,Asabim K,Nakano T.Trans Iron Steel Inst Jpn,1981;21B:511 [6]Mills K C,Billany T J H,Normanton A S.Ironmaking Steelmaking,1991;18:253 [7]Zhang J M,Zhang L,Wang X H,Wang L F.Acta Metall Sin,2003;39:1285(张炯明,张立,王新华,王立峰.金属学报,2003;39:1285) [8]Zhang X Z,Na X Z,Wang Z Y,Liu A Q,Gan Y.Acta Metall Sin,2004;40:281(张兴中,那贤昭,王忠英,刘爱强,干勇.金属学报,2004;40:281) [9]Pinheiro C A M,Samarasekera I V Brimacombe J K,Walker B N.Ironmaking Steelmaking,2000;27:37 [10]Chow C,Samarasekera I V,Walker B N,Lockhart G.Ironmaking Steelmaking,2002;29:61 [11]Yao M,Yin H B,Fang D C.ISIJ Int,2004;44:1696 [12]Savage J,Pritchard W H.Iron Steel Inst London,1954;11:260 [13]Yang H L,Zhao L G.Metall Mater Trans,1998;29B:1345 [14]Chow C,Samarasekera I V.Ironmaking Steelmaking,2002;29:53b |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|