| 车轮钢中白点及其断口研究 |
| 任学冲;褚武扬;李金许;乔利杰 |
| 北京科技大学材料科学与工程学院 |
|
| Research Of Flaking And Its Fractography In A Wheel Steel |
引用本文:
任学冲; 褚武扬; 李金许; 乔利杰 . 车轮钢中白点及其断口研究[J]. 金属学报, 2006, 42(3): 273-279 .
[1] Hirth J P. Metall Trans, 1980; 11A: 861 [2] Smialowski M. Hydrogen in Steel. New York: Pergamon Press, 1962: 327 [3] Steiner J B. Current Solution to Hydrogen Problems in Steel. Metals Park, Ohio: ASM, 1982: 55 [4] Fruehan R J. Iron Steel Maker, 1997; 24: 61 [5] Akhurst K N, Pumphreg P H. Hydrogen in Metals. Paris: Pergamon Press, 1977: 3B1 [6] Chu W Y, Gao K W, Li J X, Wang Y B, Qiao L J. Steel Res, 2001; 72: 66 [7] Pollard M G. Proc Inst Mech Eng, 1999; 213F: 181 [8] Chu W Y, Qiao L J, Chen Q Z, Gao K W. Fracture and Environment Fracture. Beijing: Science Press, 2001: 120 (褚武扬,乔利杰,陈奇志,高克玮.断裂与环境断裂,北京: 科学出版社,2001:120) [9] Andrew J H, Lee H. J Iron Steel Inst, 1947; 156: 208 [10] Chen L, Liu M Z, Yin W Q. Acta Metall Sin, 1979; 15: 446 (陈廉,刘民治,尹万全.金属学报, 1979;15:446) [11] Phillips A, Kevling V. Met Prog, 1969; 95: 81 [12] Chu W Y. Hydrogen Damage and Delayely Fracture. Beijing: Metallurgical Industry Press, 1988: 146 (褚武扬.氢损伤和滞后断裂.北京:冶金工业出版社, 1988: 146) [13] Peng X, Su Y J, Gao K W, Qiao L J, Chu W Y. Mater Lett, 2004; 58: 2073 [14] McLellan R R, Xu Z R. Scr Mater, 1997; 36: 1201 [15] Gavriljuk V G, Bugaev V N, Petrov Y N, Tarasenko A V, Yanchitski B Z. Scr Mater, 1996; 34: 903 [16] Galvele J R. Corros Set, 2004; 46: 1807 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|