Si原子择优占位对R2Co17化合物中Co次晶格磁晶各向异性的影响
胡社军 刘正义
广东工业大学机械工程系; 广州 510643
引用本文:

胡社军; 刘正义 . Si原子择优占位对R2Co17化合物中Co次晶格磁晶各向异性的影响[J]. 金属学报, 2000, 36(6): 584-588 .

全文: PDF(165 KB)  
摘要: 对R2Co17-xSix化俣物的X射线衍射和磁性测量研究结果表明, Si原子的加入使R2Co17化合物的室温磁晶各向异性由易面转变为易轴, 各向异性常数随Si原子浓度的增加而出现在值, 重点讨论了Si原子在Co次晶格四个不同晶位择优占位与Co次晶格致晶各向异性演化的关系, 其中18h晶位对Co次晶格各向异性负贡献起重要作用.
关键词 : R2Co17化合物,  磁晶各向异性    
Key words:
收稿日期: 1999-11-01     
ZTFLH:  TM273.014  
[1] Hu S J, Wei X Z, Zeng D C, Kou X C, Liu Z Y, Br 0 ckE, Klaasse J C P, de Boer F R, Buschow K H J. J AlloysCowt, 1999; 283: 83
[2] Zhang S Y, Shen B G, Liang B, Cheng Z H, Zhang J X,Zhang H W, Zhao J G, Zhan W S. J Alloys COmpds, 1998;264: 19
[3] Liang B, Shen B G, Wang F W, Zhang S Y, Zhao T J,Cheng Z H. Zhan W S. J Phys D: Appl Phys, 1998; 31:742
[4] Capehart T W, Mishra R K, Meisner G P, Fuerst C D,Herbst J F. APPl Phys Lett, 1993; 63: 362
[5] Callen H B, Callen E. J Phys Chem Sol, 1966; 27: 1271
[6] Inomata K. Phys Rev, 1981; 23B: 2076
[7] Streever R L. Phys Rev, 1979; 19B. 2704
[8] Moze O, Giovanelli L, Kockelmann W, de Groot C H, deBoer F R, Buschow K H J. J Alloys Compds, 1998; 264:76
[9] Hu Z, Yelon W B, Mishra S R, Long G J, Pringle O A,Middleton D P, Buschow K H J, Grand jean F. J ApplPhyB, 1994; 76: 443
[10] Pan Q W. J Phys: CondenB Matter, 1996; 8: 1485
[11] de Groot C H, de Boer F R, Buschow K H J, Hu Z, YelonW B. J Alloys Compds, 1996; 233: 188
[12] Marasingle G K, Mishra S R, Pringle O A, Long G J, HuZ, Yelon W B, Grand jean F, Middleton D P, Buschow KH J. J Appl Phys, 1994; 76: 6731
[13] Long G J, Narasinghe G K, Mishra S R, Pring1e O A, HuZ, Yelon W B, Middleton D P, Buschow K H J, Grand jeanF. J Appl Phys, 1994; 76. 5383
[14] Mishra S R, Long G J, Pringle O A, Hu Z, Yelon W B,Grandjean F, Buschow K H J. i Appl Phy8, 1996, 79.3145
[15] Cheng Z H, Shen B G, Yan Q W, Gao H Q, Chen D F,Guo C, Sun K, de Boer F R, Buschow K H J. Phys Rev,1998; 57B: 14299
[16] Middleton D P, Mishra S R, Long G J, Pringie O A, Hu Z,Yelon W B, Grand jean F, Buschow K H J. i Appl Phys,1995; 78: 5568
[17] Long G J, Pringle O A, Grand jean F, Ye lon W B, BuschowK H J. J Appl Phys, 1994; 74: 504
[18] Herbst J F, Croat J J, Lee R W, Ye lon W B. J Appl Phys,1982; 53. 250
[19] Hu S J, Wei X Z, Zeng D C, Kou X C, Liu Z Y, Brhck E,de Boer F R, Buschow K H J. i Magn Magn MateT, l999;196-197: 707
[20] Perkins R S, Strassler S. Phys Rev, 1977; 15B' 477
[1] 陈立彪 朱小溪 李川 刘敬华 蒋成保 徐惠彬. Fe81Ga19合金<001>取向单晶生长及磁致伸缩性能[J]. 金属学报, 2011, 47(2): 169-172.
[2] 崔跃 蒋成保 徐惠彬. Tb-Dy-Fe-Co合金本征磁致伸缩性能[J]. 金属学报, 2011, 47(2): 214-218.