| 组织细化的控制相变技术机理研究 |
| 王学敏 尚成嘉 杨善武 贺信莱 |
| 北京科技大学材料物理系;北京100083 |
|
引用本文:
王学敏; 尚成嘉; 杨善武; 贺信莱 . 组织细化的控制相变技术机理研究[J]. 金属学报, 2002, 38(6): 661-666 .
[1] Maki T. In: Taylor K A, Thompson S W, Fletched F B eds, Physical Metallurgy of Direct-Quenched Steels, War-rendale: TMS, 1993: 3 [2] Tomoya K, Keniti A, Makoto T. In: Taylor K A, Thompson S W, Fletched F B eds, Physical metallurgy of direct-quenched steels, Warrendale: TMS, 1993: 297 [3] Ernest J Czyryca, Richard E Link. Naval Eng J, May 1990: 63 [4] Shang C, Yang S, Yuan Y, He X. Thermec 2000, North-Holland, LasVegas: pergamon, 2000: 27 [5] Yang S, Shang C, Yuan Y, He X. Thermec 2000, North-Holland, LasVegas: pergamon, 2000: 25 [6] Yang S, Shang C, Yuan Y, He X. Thermec 2000, North-Holland, LasVegas: pergamon, 2000: 31 [7] Shang C, Yang S, Wang X, Yuan Y, He X. In: Liu G, Wang F, Wang Z, Zhang H eds, HSLA Steels 2000, Bei jing: Metallurgy Industry Press, 2000: 304 [8] Zhou G, Wen M, Li P, He X. Ada Metall Sin (English Lett), 2000; 13: 623 [9] Yang S, Shang C, Wang X, Yuan Y, He X. In: Liu G, Wang F, Wang Z, Zhang H eds, HSLA Steels' 2000, Bei jing: Metallurgy Industry Press, 2000: 227h |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|