| 大晶粒Ni-45Al合金的超塑性 |
| 蒋冬梅;林栋梁 |
| 上海交通大学材料和学与工程学院教育部高温材料及高温测试开放实验室; 上海 200030 |
|
| Superplasticity of Large-Grained Ni-45Al |
| JIANG Dongmei; LIN Dongliang |
| Open Laboratory of Education Ministry of China for High Temperature Materials and Tests; School of Materials Science and Engineering; Shanghai Jiaotong University; Shanghai 200030 |
引用本文:
蒋冬梅; 林栋梁 . 大晶粒Ni-45Al合金的超塑性[J]. 金属学报, 2003, 39(1): 47-50 .
,
.
Superplasticity of Large-Grained Ni-45Al[J]. Acta Metall Sin, 2003, 39(1): 47-50 .
[1] Lin D L, Shan A D, Li D Q. Scr Metall Mater, 1994; 31:1455 [2] Li D Q, Shan A D, Liu Y, Li D L. Scr Metall Mater, 1995;33: 681 [3] Lin D L, Shan A D, Chen M W. Intermetallics, 1996; 4:489 [4] Liu Y, Li D Q, Lin D L. Scr Metall Mater, 1996; 34: 1095 [5] Lin D L, Liu Y. Mater Sci Eng, 1999; A268: 83 [6] Gu Y F, Lin D L, Shan A D, Liu Y, Liu Z Y. Ada MetallSin, 1997; 33: 325(谷月峰,林栋梁,单爱党,刘毅,刘震云.金属学报,1997;33:325) [7] Liu Z Y, Lin D L,Gu Y F, Cao P,Lie C M, Huang B Y. Ada Metall Sin, 1996; 32: 1139(刘震云,林栋梁,谷月峰,曹鹏,雷长明,黄伯云.金属学报,1996;33:1139) [8] Sun F, Lin D L. Scr Mater, 2001; 44: 665 [9] Du X H, Guo J T, Zhou B D. Scr Mater, 2001; 45: 69 [10] Jiang D M, Lin D L. Mater Sci Lett, in press [11] Kim W Y, Hanada S, Sakai T. Mater Sci Eng, 1998; A248: 78 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|