| 硬状态钢铁材料磨削影响层硬化的表征 |
| 马素媛; 徐建辉; 贺笑春; 覃明; 李家宝 |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室; 沈阳 110016 |
|
| On the Characterization of Hardening of Grinding Affected Layer of Steels in Hard State |
| MA Suyuan; XU Jianhui; HE Xiaochun; QIN Ming; LI Jiabao |
| Shenyang National Laboratory for Materials Science; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
马素媛; 徐建辉; 贺笑春; 覃明; 李家宝 . 硬状态钢铁材料磨削影响层硬化的表征[J]. 金属学报, 2003, 39(2): 168-171 .
,
,
,
,
.
On the Characterization of Hardening of Grinding Affected Layer of Steels in Hard State[J]. Acta Metall Sin, 2003, 39(2): 168-171 .
[1] Meng S N. Machining Technology Handbook. Vol 1, Beijing: Machinery Industry Press, 1991; 4: 24(孟少农,机械加工工艺手册,第一卷,北京:机械工业出版社,1991;4:24) [2] Pina J P, Dias A M, Lebrun J L. In: Beck G, Denis S, Simon A eds., Proc 2nd Int Conf on Residual Stresses, London: Elsevier Applied Science, 1989: 690 [3] Ji N, Lebrun J L, Belliard P, Bourniquel B, Maeder G. In: Beck G, Denis S, Simon A eds., Proc 2nd Int Conf on Residual Stresses, London: Elsevier Applied Science, 1989: 65 [4] Li J B, Xu H B, Chen R, Wang Z G. Metall Mater Trans, 1996; 27A: 3662 [5] Xu H B. Thesis of Masters' Degree, Shenyang, Institute of Metal Research, The Chinese Academy of Sciences, 1997(徐寒冰.中国科学院金属研究所硕士学位论文,沈阳, 1997) [6] Burgahn F, Vohringer O, Macherauch E. In: lida K ed., Proc. 4th Int Conf on Shot Peening, Tokyo: Japan Society of Precision Engineering, 1990: 199 [7] Wang W H. Thesis of Masters' Degree, Shenyang, Institute of Metal Research, The Chinese Academy of Sciences, 1999(王文洪.中国科学院金属研究所硕士学位论文,沈阳, 1999) [8] Ashby M F, Jones D R H. Engineering Materials. Oxford:Pergamon Press, 1980: 105 [9] Tan M T. Microscopic Study of Metal Cutting. Shanghai:Science and Technology Press, 1988: 207(谭美田,金属切削微观研究.上海:上海科学技术出版社,1988:207) [10] Yonetani S, Translated by Zhu J P, Shao H M. Produce and Counter-measure of Residual Stress. Beijing: Machinery Industry Press, 1983: 180(米谷茂(日)著,朱荆璞,邵会孟译,残余应力的产生与对策北京:机械工业出版社, 1983:180) [11] Hilley M E, Larson J A, Jatczak C F, Ricklefs R E. Residual Stress Measurement by X-ray Diffraction. Society of Automotive Engineers Information R,eport, No. J784a, 1971: 5 [12] Macherauch E, Wohlfahrt H. Wolfstieg U. Harterei Technol Mit, 1973; 28: 201 [13] Hauk V. Residual Stresses. Oberursel: ERG, DGM-Informationsgesellschaft, 1986: 9P |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|