Please wait a minute...
金属学报  2003, Vol. 39 Issue (2): 168-171     
  论文 本期目录 | 过刊浏览 |
硬状态钢铁材料磨削影响层硬化的表征
马素媛; 徐建辉; 贺笑春; 覃明; 李家宝
中国科学院金属研究所沈阳材料科学国家(联合)实验室; 沈阳 110016
On the Characterization of Hardening of Grinding Affected Layer of Steels in Hard State
MA Suyuan; XU Jianhui; HE Xiaochun; QIN Ming; LI Jiabao
Shenyang National Laboratory for Materials Science; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016
引用本文:

马素媛; 徐建辉; 贺笑春; 覃明; 李家宝 . 硬状态钢铁材料磨削影响层硬化的表征[J]. 金属学报, 2003, 39(2): 168-171 .
, , , , . On the Characterization of Hardening of Grinding Affected Layer of Steels in Hard State[J]. Acta Metall Sin, 2003, 39(2): 168-171 .

全文: PDF(188 KB)  
摘要: 显微硬度和X射线衍射线半高宽常被用来表征强化表面的静强度及其在强化表面层内的分布. 然而实验结果表明, 对于两种经过磨削加工的硬状态钢铁材料, 磨削塑性形变虽使其表层的显微硬度明显提高, 却使其半高宽值大幅度减小. 因此, X射线衍射线的半高宽不能正确的反映硬状态钢铁材料磨削影响层的强化效果。文中利用一个模型和X射线衍射线的线形分析结果来说明磨削塑性形变是通过降低微观应力从而使半高宽减小的.
关键词 : 钢铁材料,  半高宽,  磨削    
Key words:
收稿日期: 2002-08-27     
ZTFLH:  TG142  
[1] Meng S N. Machining Technology Handbook. Vol 1, Beijing: Machinery Industry Press, 1991; 4: 24(孟少农,机械加工工艺手册,第一卷,北京:机械工业出版社,1991;4:24)
[2] Pina J P, Dias A M, Lebrun J L. In: Beck G, Denis S, Simon A eds., Proc 2nd Int Conf on Residual Stresses, London: Elsevier Applied Science, 1989: 690
[3] Ji N, Lebrun J L, Belliard P, Bourniquel B, Maeder G. In: Beck G, Denis S, Simon A eds., Proc 2nd Int Conf on Residual Stresses, London: Elsevier Applied Science, 1989: 65
[4] Li J B, Xu H B, Chen R, Wang Z G. Metall Mater Trans, 1996; 27A: 3662
[5] Xu H B. Thesis of Masters' Degree, Shenyang, Institute of Metal Research, The Chinese Academy of Sciences, 1997(徐寒冰.中国科学院金属研究所硕士学位论文,沈阳, 1997)
[6] Burgahn F, Vohringer O, Macherauch E. In: lida K ed., Proc. 4th Int Conf on Shot Peening, Tokyo: Japan Society of Precision Engineering, 1990: 199
[7] Wang W H. Thesis of Masters' Degree, Shenyang, Institute of Metal Research, The Chinese Academy of Sciences, 1999(王文洪.中国科学院金属研究所硕士学位论文,沈阳, 1999)
[8] Ashby M F, Jones D R H. Engineering Materials. Oxford:Pergamon Press, 1980: 105
[9] Tan M T. Microscopic Study of Metal Cutting. Shanghai:Science and Technology Press, 1988: 207(谭美田,金属切削微观研究.上海:上海科学技术出版社,1988:207)
[10] Yonetani S, Translated by Zhu J P, Shao H M. Produce and Counter-measure of Residual Stress. Beijing: Machinery Industry Press, 1983: 180(米谷茂(日)著,朱荆璞,邵会孟译,残余应力的产生与对策北京:机械工业出版社, 1983:180)
[11] Hilley M E, Larson J A, Jatczak C F, Ricklefs R E. Residual Stress Measurement by X-ray Diffraction. Society of Automotive Engineers Information R,eport, No. J784a, 1971: 5
[12] Macherauch E, Wohlfahrt H. Wolfstieg U. Harterei Technol Mit, 1973; 28: 201
[13] Hauk V. Residual Stresses. Oberursel: ERG, DGM-Informationsgesellschaft, 1986: 9P
[1] 徐伟,黄明浩,王金亮,沈春光,张天宇,王晨充. 综述:钢中亚稳奥氏体组织与疲劳性能关系[J]. 金属学报, 2020, 56(4): 459-475.
[2] 罗庆洪 李春志 娄艳芝 赵振业. 磨削工艺对渗碳M50NiL钢表面变质层微观结构和性能及疲劳性能影响[J]. 金属学报, 2012, 48(2): 194-198.
[3] 章晓中; 张丽娜; 马钺; 齐俊杰; 袁俊 . 钢铁材料晶界性质和冲击断裂特征的电子结构表征[J]. 金属学报, 2005, 41(6): 617-621 .