| 传输线模型分析有机涂层厚度对阻抗谱的影响 |
| 孙秋霞; 张鉴清; 林薇薇 |
| (浙江大学化学系; 杭州 310013) |
|
引用本文:
孙秋霞; 张鉴清; 林薇薇 . 传输线模型分析有机涂层厚度对阻抗谱的影响[J]. 金属学报, 2004, 40(11): 1205-1209 .
[1] Cao C N, Zhang J Q. An Introduction to Electrochemical Impedance Spectroscopy, Beijing: Science Press, 2002(曹楚南,张鉴清.电化学阻抗谱导论,北京:科学出版社,2002) [2] Hirayamas R, Haruyama S, Corrosion, 1991; 47: 952 [3] Fedrizzi L, Deflorian F, Bonora P L. Electrochim Acta,1999; 44(24) : 4251 [4] Deflorian F, Fedrizzi L, Bonora P L. Prog Org Coat, 1993;23: 73 [5] Pebere N, Picaud T H, Duprat M, Dabosi F. Corros Sci,1989; 29: 1073 [6] Mansfeld F, Kendig M W, Tsai S. Corrosion, 1982; 38:570 [7] Grandle J A, Taylor S R. Corrosion, 1997; 53 (5) : 347 [8] Brasher D M, Kingsbury A H. J Appl Chem, 1954; 4: 62 [9] Gonzalez S, Gil M A, Hernandez J O, Fox V, Sout R M.Prog Org Coat, 2001; 41: 167 [10] Sun Q X, Zhang J Q, Lin O J. Acta Phys-Chim Sin, 2004;1: 70(孙秋霞,张鉴清,林昌健.物理化学学报, 2004;1:70) [11] Santagtate D M, Rere P R, Eisner C I, Di Sarli A R. ProgOrg Coat, 1998; 33: 44 [12] Domingues L, Oliveira C, Fernandes J C S, Ferreira M GS. Electrochim Acta, 2002; 47(13-14) : 2253 [13] Campestrini P, van Westing E P M,de Wit J H W. Electrochim Acta, 2001; 46: 2631 [14] Jimenez-Morales A, Galvan J C, Aranda P A. ElectrochimActa, 2002; 47: 2281 [15] Liu B, Li Y, Lin H C, Cao C N. Corros Sci, 2002; 44:2657 [16] Deflorian F, Fedrizzi L, Rossi S. Corrosion, 1999; 55: 1003 [17] Deflorian F, Fedrizzi L. J Adhesion Sci Technol, 1999;13(5) : 629 [18] van Westing E P M, Ferrari G M, de Wit J H. Corros Sci,1994; 36(6) : 957 [19] Kendig M W. Corrosion, 1999; 55: 222 [20] Miskovic-Stankovic V B, Drazic D M, Kacarevic-PopovicZ. Corros Sci, 1996; 38: 1513 [21] Shigeyoshi M, Prog Org Coat, 1996; 28: 227 [22] Fedrizzi L, Rodriguez F J, Rossi S, Deflorian F, Di MaggioR. Electrochim Acta, 2001; 46: 3715 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|