					引用本文:
						|  |  
    					|  |  
    					| 球磨诱发AlN陶瓷微观结构的演变 |  
						| 杨志卿  贺连龙  金志雄  叶恒强 |  
					| 中国科学院金属研究所固体原子像开放研究实验室;沈阳110015 |  
						|  |  
								杨志卿; 贺连龙; 金志雄; 叶恒强                                                                                                                                                                                                                                    . 球磨诱发AlN陶瓷微观结构的演变[J]. 金属学报, 2001, 37(3): 230-234       .	
																												 
					
						| 
								
									|  
          
          
            
                         
            
									            
									                
																														  
																| [1] Benjamin J S. Matall Mater, 1970; 1: 2493 [2] Fecht H J, Hellstern E, Fu Z, Johnson W L. Metall Trans,1990; 21A: 2333
 [3] Hellstern E, Fecht H J, Fu Z, Johbnson W L. J Appl Phys,1989; 65: 305
 [4] Fecht H J. Nanostruct. Mater, 1995; 6: 33
 [5] Kimura H, Kimura M, Takada F. J Less-common Metals,1988; 140: 113
 [6] Yang X Y, Wu Y K, Ye H Q. Philosph Mag Lett, 2000;80: 333
 [7] Huang J Y, Yasuda H, Mori H. Philosph Mag Lett, 1999;79: 305
 [8] Pezzotti G, Lee B T. Hiraga K. J Mater Sci, 1994; 29:1786
 [9] Lee B T, Hiraga K. i Mater Res, 1994; 9: 1199
 [10] Lee B T, Nishiyama A, Hiraga K. Mater Trans, 199JIM34: 682
 [11] Edgar J H. J Mater Res, 1992; 7: 235
 [12] Mroz T J. Ceram Bull, 1992; 71: 782
 [13] Masson I, Feiereisen J P, Michel J P, Mocellin A, GuenalC. Br. Ceram Trans J, 1992; 91: 177
 [14] Seifert A, Berger A, Muller W F. J Am Ceram Soc, 19975: 873
 [15] Audurier V, Demenet J L, Rabier J. Philosph Mag, 1998A77: 825
 [16] Audurier V, Demenet J L, Rabier J. Philosph Mag, 1998A77: 843
 [17] Jiang J S C, Koch C C. J Mater Res, 1990; 5: 498
 [18] Schwarz R B, Johnson W L. J Less-Common Met, 1988140: 1
 |  
             
												
											    	
											        	|  | Viewed |  
											        	|  |  |  
												        |  | Full text 
 | 
 
 |  
												        |  |  |  
												        |  | Abstract 
 | 
 |  
												        |  |  |  
												        |  | Cited |  |  
												        |  |  |  |  
													    |  | Shared |  |  
													    |  |  |  |  
													    |  | Discussed |  |  |  |  |