| 高 γ′相含量GH4151变形高温合金铸态组织与开裂敏感性分析 |
钟佳, 王法, 江河, 姚志浩, 董建新( ) |
| 北京科技大学 材料科学与工程学院 北京 100083 |
|
| Analyses of As-Cast Microstructure and Cracking Sensitivity of GH4151 Wrought Superalloy with High γ′ Phase Content |
ZHONG Jia, WANG Fa, JIANG He, YAO Zhihao, DONG Jianxin( ) |
| School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China |
引用本文:
钟佳, 王法, 江河, 姚志浩, 董建新. 高 γ′相含量GH4151变形高温合金铸态组织与开裂敏感性分析[J]. 金属学报, 2025, 61(11): 1653-1663.
Jia ZHONG,
Fa WANG,
He JIANG,
Zhihao YAO,
Jianxin DONG.
Analyses of As-Cast Microstructure and Cracking Sensitivity of GH4151 Wrought Superalloy with High γ′ Phase Content[J]. Acta Metall Sin, 2025, 61(11): 1653-1663.
| [1] |
Wang F. The influence of characteristics due to high-content γ′ on microstructures and properties of difficult-to-deform GH4151 alloy and the exploration of alloys with higher service temperature [D]. Beijing: University of Science and Technology Beijing, 2023
|
| [1] |
王 法. 高含量γ′特性对难变形GH4151合金组织性能影响及更高使用温度合金探索 [D]. 北京: 北京科技大学, 2023
|
| [2] |
Zhang J, Wang L, Xie G, et al. Recent progress in research and development of nickel-based single crystal superalloys [J]. Acta Metall. Sin., 2023, 59: 1109
|
| [2] |
张 健, 王 莉, 谢 光 等. 镍基单晶高温合金的研发进展 [J]. 金属学报, 2023, 59: 1109
|
| [3] |
Yin B, Xie G, Lou L H, et al. Abnormal increase of TCP phase during heat treatment in a Ni-based single crystal superalloy [J]. Scr. Mater., 2019, 173: 1
|
| [4] |
Xu Z Q, Yang S F, Zhao P, et al. Phase precipitation and segregation behavior of nickel-based superalloy GH4151 [J]. J. Iron Steel Res., 2022, 34: 588
|
| [4] |
徐志强, 杨树峰, 赵 朋 等. 镍基高温合金GH4151的偏析及相析出行为 [J]. 钢铁研究学报, 2022, 34: 588
|
| [5] |
Li X X, Jia C L, Zhang Y, et al. Cracking mechanism in as-cast GH4151 superalloy ingot with high γ′ phase content [J]. Trans. Nonferrous Met. Soc. China, 2020, 30: 2697
|
| [6] |
Lv S M, Chen J B, He X B, et al. Investigation on sub-solvus recrystallization mechanisms in an advanced γ-γ′ nickel-based superalloy GH4151 [J]. Materials, 2020, 13: 4553
|
| [7] |
Bi Z N, Qu J L, Du J H, et al. Microstructure characteristics and thermodynamic calculation of equilibrium precipitated phases in a new difficult-to-deform superalloy эк151 [J]. Rare Met. Mater. Eng., 2013, 42: 919
|
| [7] |
毕中南, 曲敬龙, 杜金辉 等. 新型难变形高温合金эк151的组织特征及平衡析出相热力学计算 [J]. 稀有金属材料与工程, 2013, 42: 919
|
| [8] |
Bi Z N, Qu J L, Du J H, et al. Segregation behavior and investigation on homogenization for a new difficult-to-deform superalloy ЭК151 ingot [J]. J. Iron Steel Res., 2011, 23(suppl.2): 263
|
| [8] |
毕中南, 曲敬龙, 杜金辉 等. 新型难变形高温合金ЭК151的偏析行为及均匀化工艺研究 [J]. 钢铁研究学报, 2011, 23(): 263
|
| [9] |
Zhao Z, Dong J X, Zhang M C, et al. Microstructure and susceptibility to hot tearing of K424 nickel-based superalloys for turbocharger turbine wheels [J]. Chin. J. Eng., 2016, 38: 1429
|
| [9] |
赵 展, 董建新, 张麦仓 等. 增压涡轮用K424高温合金组织特征及热裂倾向性 [J]. 工程科学学报, 2016, 38: 1429
|
| [10] |
Zhao Z, Dong J X, Zhang M C, et al. Solidification characteristics and microstructures evolution of Ni-based superalloy K424 with different solidification cooling rates [J]. Chin. J. Eng., 2018, 40: 1332
|
| [10] |
赵 展, 董建新, 张麦仓 等. K424高温合金凝固特征及冷却速度对其影响规律 [J]. 工程科学学报, 2018, 40: 1332
|
| [11] |
Zhao Z. Influences and control of microstructures and process on hot-tearing for superalloy turbocharger turbine wheels [D]. Beijing: University of Science and Technology Beijing, 2020
|
| [11] |
赵 展. 增压涡轮用高温合金组织和工艺对热裂的影响与控制 [D]. 北京: 北京科技大学, 2020
|
| [12] |
Xu J J, Lin X, Guo P F, et al. The initiation and propagation mechanism of the overlapping zone cracking during laser solid forming of IN-738LC superalloy [J]. J. Alloys Compd., 2018, 749: 859
|
| [13] |
Zhou Y Z, Volek A, Singer R F. Effect of grain boundary characteristics on hot tearing in directional solidification of superalloys [J]. J. Mater. Res., 2006, 21: 2361
|
| [14] |
Fojt-Dymara G, Opiela M, Borek W. Susceptibility of high-manganese steel to high-temperature cracking [J]. Materials, 2022, 15: 8198
|
| [15] |
Jia L, Cui H, Yang S F, et al. The cracking behavior of the new Ni-based superalloy GH4151 in the triple melting process [J]. J. Mater. Res. Technol., 2023, 25: 2368
|
| [16] |
Lv S M, Jia C L, He X B, et al. Superplastic deformation and dynamic recrystallization of a novel disc superalloy GH4151 [J]. Materials, 2019, 12: 3667
|
| [17] |
Tan Y G. Investigation of solidification and high-temperature deformation behavior of Ni-base alloy ЭК151 [D]. Hefei: University of Science and Technology of China, 2019
|
| [17] |
谭远过. 新型镍基高温合金ЭК151凝固偏析及高温变形行为研究 [D]. 合肥: 中国科学技术大学, 2019
|
| [18] |
Tan Y G, Liu F, Zhang A W, et al. Element segregation and solidification behavior of a Nb, Ti, Al Co-strengthened superalloy ЭК151 [J]. Acta Metall. Sin. (Engl. Lett.), 2019, 32: 1298
|
| [19] |
Kong D C, Dong C F, Ni X Q, et al. High-throughput fabrication of nickel-based alloys with different Nb contents via a dual-feed additive manufacturing system: Effect of Nb content on microstructural and mechanical properties [J]. J. Alloys Compd., 2019, 785: 826
|
| [20] |
Jiang H, Nai Q L, Xu C, et al. Sensitive temperature and reason of rapid fatigue crack propagation in nickel-based superalloy [J]. Acta Metall. Sin., 2023, 59: 1190
|
| [20] |
江 河, 佴启亮, 徐 超 等. 镍基高温合金疲劳裂纹急速扩展敏感温度及成因 [J]. 金属学报, 2023, 59: 1190
|
| [21] |
Li Y S, Dong Y W, Jiang Z H, et al. Study on microsegregation and homogenization process of a novel nickel-based wrought superalloy [J]. J. Mater. Res. Technol., 2022, 19: 3366
|
| [22] |
Bi Z N, Qin H L, Dong Z G, et al. Residual stress evolution and its mechanism during the manufacture of superalloy disk forgings [J]. Acta Metall. Sin., 2019, 55: 1160
|
| [22] |
毕中南, 秦海龙, 董志国 等. 高温合金盘锻件制备过程残余应力的演化规律及机制 [J]. 金属学报, 2019, 55: 1160
|
| [23] |
Zhou H, Wang P, Lu S P. Effect of grain boundary morphology and MC on plastic deformation behavior of NiCrFe weld metal: Crystal plasticity finite element analysis [J]. Chin. J. Mater. Res., 2019, 33: 801
|
| [23] |
周 辉, 王 培, 陆善平. NiCrFe焊缝金属的晶界形貌和晶界MC碳化物对局部变形行为的影响 [J]. 材料研究学报, 2019, 33: 801
|
| [24] |
Wu Y S. Effect of phosphorus on the deformation behavior of GH984G alloy [D]. Hefei: University of Science and Technology of China, 2020
|
| [24] |
吴云胜. 磷含量对GH984G合金变形行为的影响 [D]. 合肥: 中国科学技术大学, 2020
|
| [25] |
Lu N N, Guo Y M, Yang S L, et al. Formation mechanisms of hot cracks in laser additive repairing single crystal superalloys [J]. Acta Metall. Sin., 2023, 59: 1243
|
| [25] |
卢楠楠, 郭以沫, 杨树林 等. 激光增材修复单晶高温合金的热裂纹形成机制 [J]. 金属学报, 2023, 59: 1243
|
| [26] |
Wang X Q, Gong X B, Chou K. Review on powder-bed laser additive manufacturing of Inconel 718 parts [J]. Proc. Inst. Mech. Eng., 2017, 231B: 1890
|
| [27] |
Chen Y, Zhang K, Huang J, et al. Characterization of heat affected zone liquation cracking in laser additive manufacturing of Inconel 718 [J]. Mater. Des., 2016, 90: 586
|
| [28] |
Wang T, Wan Z P, Li Z, et al. Effect of heat treatment parameters on microstructure and hot workability of as-cast fine grain ingot of GH4720Li alloy [J]. Acta Metall. Sin., 2020, 56: 182
|
| [28] |
王 涛, 万志鹏, 李 钊 等. 热处理工艺对GH4720Li合金细晶铸锭组织与热加工性能的影响 [J]. 金属学报, 2020, 56: 182
|
| [29] |
Wang D, Liu Z, Wang J G, et al. Study on microstructure and properties of shaped ring parts for super alloy GH4738 [J]. Forg. Stamp. Technol., 2020, 45(5): 128
|
| [29] |
王 丹, 刘 智, 王建国 等. GH4738高温合金异形环件组织与性能研究 [J]. 锻压技术, 2020, 45(5): 128
|
| [30] |
Yan X F, Dong J X, Shi Z X, et al. Solidification and segregation behavior of nickel-based superalloy GH4282 [J]. Rare Met. Mater. Eng., 2019, 48: 3183
|
| [30] |
颜晓峰, 董建新, 石照夏 等. 镍基高温合金GH4282的凝固和偏析行为 [J]. 稀有金属材料与工程, 2019, 48: 3183
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|