| 超声共混合成Ni(HNCN)2/BiVO4复合可见光催化剂 |
张霞( ), 宋扬, 王誉, 纪逯鹤, 杨媚, 孟皓 |
| 东北大学理学院化学系 沈阳 110819 |
|
| Ultrasonic Blending Synthesis of Ni(HNCN)2/BiVO4 Composite Visible-Light Induced Photocatalysts |
ZHANG Xia( ), SONG Yang, WANG Yu, JI Luhe, YANG Mei, MENG Hao |
| Faculty of Chemistry, College of Sciences, Northeastern University, Shenyang 110819, China |
引用本文:
张霞, 宋扬, 王誉, 纪逯鹤, 杨媚, 孟皓. 超声共混合成Ni(HNCN)2/BiVO4复合可见光催化剂[J]. 金属学报, 2020, 56(11): 1551-1557.
Xia ZHANG,
Yang SONG,
Yu WANG,
Luhe JI,
Mei YANG,
Hao MENG.
Ultrasonic Blending Synthesis of Ni(HNCN)2/BiVO4 Composite Visible-Light Induced Photocatalysts[J]. Acta Metall Sin, 2020, 56(11): 1551-1557.
| [1] |
Le Moal M, Gascuel-Odoux C, Ménesguen A, et al. Eutrophication: A new wine in an old bottle? [J]. Sci. Total Environ., 2019, 651: 1
doi: 10.1016/j.scitotenv.2018.09.139
pmid: 30223216
|
| [2] |
Fujishima A, Honda K. Electrochemical photolysis of water at a semiconductor electrode [J]. Nature, 1972, 238: 37
pmid: 12635268
|
| [3] |
Ding Y, Yang I S, Li Z Q, et al. Nanoporous TiO2 spheres with tailored textural properties: Controllable synthesis, formation mechanism, and photochemical applications [J]. Prog. Mater. Sci., 2020, 109: 100620
|
| [4] |
Katal R, Masudy-Panah S, Tanhaei M, et al. A review on the synthesis of the various types of anatase TiO2 facets and their applications for photocatalysis [J]. Chem. Eng. J., 2020, 384: 123384
|
| [5] |
Di T M, Xu Q L, Ho W K, et al. Review on metal sulphide-based Z-scheme photocatalysts [J]. ChemCatChem, 2019, 11: 1394
|
| [6] |
Tayebi M, Lee B K. Recent advances in BiVO4 semiconductor materials for hydrogen production using photoelectrochemical water splitting [J]. Renew. Sustain. Energy Rev., 2019, 111: 332
|
| [7] |
Wang T, Nie C Y, Ao Z M, et al. Recent progress in g-C3N4 quantum dots: Synthesis, properties and applications in photocatalytic degradation of organic pollutants [J]. J. Mater. Chem., 2020, 8A: 485
|
| [8] |
Mun S J, Park S J. Graphitic carbon nitride materials for photocatalytic hydrogen production via water splitting: A short review [J]. Catalysts, 2019, 9: 805
|
| [9] |
Wang X C, Maeda K, Thomas A, et al. A metal-free polymeric photocatalyst for hydrogen production from water under visible light [J]. Nat. Mater., 2009, 8: 76
pmid: 18997776
|
| [10] |
Tian K, Liu W J, Jiang H. Comparative investigation on photoreactivity and mechanism of biogenic and chemosythetic Ag/C3N4 composites under visible light irradiation [J]. ACS Sustainable Chem. Eng., 2015, 3: 269
|
| [11] |
Deb S K, Yoffe A D. Inorganic cyanamides. Physical and optical properties, and decomposition [J]. Trans. Faraday Soc., 1959, 55: 106
doi: 10.1039/tf9595500106
|
| [12] |
Liu X H, Krott M, Müller P, et al. Synthesis, crystal structure, and properties of MnNCN, the first carbodiimide of a magnetic transition metal [J]. Inorg. Chem., 2005, 44: 3001
pmid: 15847401
|
| [13] |
Liu X H, Stork L, Speldrich M, et al. FeNCN and Fe(NCNH)2: Synthesis, structure, and magnetic properties of a nitrogen-based pseudo-oxide and -hydroxide of divalent iron [J]. Chem. Eur. J., 2009, 15: 1558
pmid: 19115292
|
| [14] |
Krott M, Liu X H, Fokwa B P T, et al. Synthesis, crystal-structure determination and magnetic properties of two new transition-metal carbodiimides: CoNCN and NiNCN [J]. Inorg. Chem., 2007, 46: 2204
doi: 10.1021/ic062051o
pmid: 17302407
|
| [15] |
Zhao W, Liu Y F, Liu J J, et al. Controllable synthesis of silver cyanamide as a new semiconductor photocatalyst under visible-light irradiation [J]. J. Mater. Chem., 2013, 1A: 7942
|
| [16] |
Schädler H D, Jäger L, Senf I. Pseudoelementverbindungen. V. Pseudochalkogene—Versuch der empirischen und theoretischen Charakterisierung eines Konzeptes [J]. Z. Anorg. Allg. Chem., 1993, 619: 1115
|
| [17] |
Meng H, Li X X, Zhang X, et al. Fabrication of nanocomposites composed of silver cyanamide and titania for improved photocatalytic hydrogen generation [J]. Dalton Trans., 2015, 44: 19948
pmid: 26515664
|
| [18] |
Meng X R, Yao P, Xu Y, et al. Fabrication of organic-inorganic hybrid membranes composed of poly (vinylidene fluoride) and silver cyanamide and their high photocatalytic activity under visible light irradiation [J]. RSC Adv., 2016, 6: 61920
doi: 10.1039/C6RA10434G
|
| [19] |
Rong F F, Wang Y, Zhang X. Structure and visible-light induced photocatalytic activity of zinc cyanamide-based photocatalysts [J]. Acta Metall. Sin., 2018, 54: 76
doi: 10.11900/0412.1961.2017.00126
|
| [19] |
(荣凤鸣, 王 誉, 张 霞. 基于氰胺锌的复合光催化剂的结构与可见光催化性能 [J]. 金属学报, 2018, 54: 76)
doi: 10.11900/0412.1961.2017.00126
|
| [20] |
Krott M, Liu X H, Müller P, et al. Synthesis and structure determination of Co(HNCN)2 and Ni(HNCN)2 [J]. J. Solid State Chem., 2007, 180: 307
doi: 10.1016/j.jssc.2006.10.021
|
| [21] |
Kudo A, Ueda K, Kato H, et al. Photocatalytic O2 evolution under visible light irradiation on BiVO4 in aqueous AgNO3 solution [J]. Catal. Lett., 1998, 53: 229
doi: 10.1023/A:1019034728816
|
| [22] |
Liu X H, Müller P, Kroll P, et al. Synthesis, structure determination, and quantum-chemical characterization of an alternate HgNCN polymorph [J]. Inorg. Chem., 2002, 41: 4259
pmid: 12160416
|
| [23] |
Sameera S, Rao P P, Divya S, et al. High IR reflecting BiVO4-CaMoO4 based yellow pigments for cool roof applications [J]. Energy Build., 2017, 154: 491
doi: 10.1016/j.enbuild.2017.08.089
|
| [24] |
Yue X Z, Yi S S, Wang R W, et al. Cobalt phosphide modified titanium oxide nanophotocatalysts with significantly enhanced photocatalytic hydrogen evolution from water splitting [J]. Small, 2017, 13: 1603301
doi: 10.1002/smll.v13.14
|
| [25] |
Hao X Q, Wang Y C, Zhou J, et al. Zinc vacancy-promoted photocatalytic activity and photostability of ZnS for efficient visible-light-driven hydrogen evolution [J]. Appl. Catal., 2018, 221B: 302
|
| [26] |
Xiao Y J, Qi Y, Wang X L, et al. Visible-light-responsive 2D cadmium-organic framework single crystals with dual functions of water reduction and oxidation [J]. Adv. Mater., 2018, 30: 1803401
doi: 10.1002/adma.v30.44
|
| [27] |
Qiu Y C, Yan K Y, Deng H, et al. Secondary branching and nitrogen doping of ZnO nanotetrapods: Building a highly active network for photoelectrochemical water splitting [J]. Nano Lett., 2012, 12: 407
pmid: 22149105
|
| [28] |
Song H H, Sun Z Q, Xu Y, et al. Fabrication of NH2-MIL-125(Ti) incorporated TiO2 nanotube arrays composite anodes for highly efficient PEC water splitting [J]. Sep. Purif. Technol., 2019, 228: 115764
doi: 10.1016/j.seppur.2019.115764
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|