| 富Sb相对锌合金在近中性和酸性溶液中耐蚀性的影响 |
尚秀玲1,张波2( ),柯伟2 |
1 广东美的制冷设备有限公司 佛山 528311 2 中国科学院金属研究所中国科学院核用材料与安全评价重点实验室 沈阳 110016 |
|
| Effect of Sb-Rich Intermetallic Phase on the CorrosionResistance of Zn Alloy in Near-Neutral and Acidic Solutions |
Xiuling SHANG1,Bo ZHANG2( ),Wei KE2 |
1 GD Midea Air-Conditioning Equipment Co., LTD., Foshan 528311, China 2 Key Laboratory of Nuclear Materials and Safety Assessment, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China |
引用本文:
尚秀玲,张波,柯伟. 富Sb相对锌合金在近中性和酸性溶液中耐蚀性的影响[J]. 金属学报, 2017, 53(3): 351-357.
Xiuling SHANG,
Bo ZHANG,
Wei KE.
Effect of Sb-Rich Intermetallic Phase on the CorrosionResistance of Zn Alloy in Near-Neutral and Acidic Solutions[J]. Acta Metall Sin, 2017, 53(3): 351-357.
| [1] | Frydrych D J.Corrosion mechanisms of zinc-rich organic coatings on steel [D]. Pennsylvania: University of Pennsylvania, 1987 | | [2] | Zhu L.Hot Dip Galvanizing of Steels [M]. Beijing: Chemical Industry Press, 2005: 28 | | [2] | (朱立. 钢材热镀锌 [M]. 北京: 化学工业出版社, 2005: 28) | | [3] | Hosking N C, Str?m M A, Shipway P H, et al.Corrosion resistance of zinc-magnesium coated steel[J]. Corros. Sci., 2007, 49: 3669 | | [4] | Ramanauskas R, Muleshkova L, Maldonado L, et al.Characterization of the corrosion behaviour of Zn and Zn alloy electrodeposits: Atmospheric and accelerated tests[J]. Corros. Sci., 1998, 40: 401 | | [5] | Hosny A Y, El-Rafei M E, Ramadan T A, et al. Corrosion resistance of zinc coatings produced from a sulfate bath[J]. Met. Finish., 1995, 93: 55 | | [6] | Fratesi R, Roventi G, Branca C, et al.Corrosion resistance of Zn-Co alloy coatings[J]. Surf. Coat. Technol., 1994, 63: 97 | | [7] | Diaz-Ballote L, Ramanauskas R.Improving the corrosion resistance of hot dip galvanized zinc coatings by alloying[J]. Corros. Rev., 1999, 17: 411 | | [8] | Boshkov N.Galvanic Zn-Mn alloys——electrodeposition, phase composition, corrosion behaviour and protective ability[J]. Surf. Coat. Technol., 2003, 172: 217 | | [9] | Münz R, Wolf G K, Guzman L, et al.Zinc/manganese multilayer coatings for corrosion protection[J]. Thin Solid Films, 2004, 459: 297 | | [10] | Leidheiser H Jr, Suzuki I.Technical note: Towards a more corrosion resistant galvanized steel[J]. Corrosion, 1980, 36: 701 | | [11] | Shang X L, Zhang B, Han E H, et al.The effect of 0.4 wt.% Mn addition on the localized corrosion behaviour of zinc in a long-term experiment[J]. Electrochim. Acta, 2012, 65: 294 | | [12] | Shang X L, Zhang B, Han E H, et al.Effect of small addition of Mn on the passivation of Zn in 0.1M NaOH solution[J]. Electrochim. Acta, 2011, 56: 1417 | | [13] | Marder A R.The metallurgy of zinc-coated steel[J]. Prog. Mater. Sci., 2000, 45: 191 | | [14] | Zhang B, Zhou H B, Han E H, et al.Effects of a small addition of Mn on the corrosion behaviour of Zn in a mixed solution[J]. Electrochim. Acta, 2009, 54: 6598 | | [15] | Sebisty J J, Palmer R H.The influence of combined additions of tin, cadmium, antimony and copper on the structure and properties of galvanized coatings [A]. Proceedings of 6th International Conference on Hot Dip Galvanizing[C]. London: Zinc Development Association, 1961: 215 | | [16] | Fasoyino F A, Weinberg F.Spangle formation in galvanized sheet steel coatings[J]. Metall. Trans., 1990, 21B: 549 | | [17] | Rdeker W, Friehe W. Effect of alloy additions on the properties of hot galvanized coatings [A]. Proceedings of 7th International Conference on Hot Dip Galvanizing [C]. Paris: Pergamon Press, 1964: 167 | | [18] | Chang S, Shin J C.The effect of antimony additions on hot dip galvanized coatings[J]. Corros. Sci., 1994, 36: 1425 | | [19] | Hansen M, Elliott R P, Shunk F A.Constitution of Binary Alloys[M]. New York: McGraw-Hill Book Co., 1958: 1 | | [20] | Hanna F, Nassif N.Factors affecting the quality of hot-dip-galvanized steel sheets[J]. Surf. Technol., 1984, 21: 27 | | [21] | Adjadj F, Belbacha E D, Bouharkat M, et al.Crystallographic study of the intermediate compounds SbZn, Sb3Zn4 and Sb2Zn3[J]. J. Alloys Compd., 2006, 419: 267 | | [22] | Izard V, Record M C, Tedenac J C.Mechanical alloying of a new promising thermoelectric material, Sb3Zn4[J]. J. Alloys Compd., 2002, 345: 257 | | [23] | El-Egamy S S. Electrochemical behavior of antimony and antimony oxide films in acid solutions[J]. Corrosion, 2006, 62: 739 | | [24] | Cané E, Fusina L, Tarroni R, et al.High resolution infrared study of SbHD2: The ground state and the Sb-H stretching bands v1 and 2v1[J]. J. Mol. Spectrosc., 2011, 265: 1 | | [25] | Xu R, Ma K, Guo Z.Activation mechanism of Sb2O3 during removal of cobalt from zinc sulphate solution[J]. Hydrometallurgy, 2006, 82: 150 | | [26] | Li H, Zhang B, Wang J Q, et al.Effect of Sb and Mn additions on the corrosion behaviour of Zn[J]. J. Chin. Soc. Corros. Prot., 2008, 28: 257 | | [26] | (李红, 张波, 王俭秋等. 合金元素Sb和Mn对Zn腐蚀的影响. 中国腐蚀与防护学报, 2008, 28: 257) |
|
|