|
|
|
| 水合肼制氢Ni-Pt/La2O3催化剂研制及其反应动力学研究* |
钟玉洁1,戴洪斌2( ),王平2 |
1 中国科学院金属研究所, 沈阳 110016 2 华南理工大学材料科学与工程学院广东省先进储能重点实验室, 广州510641 |
|
| PREPARATION OF Ni-Pt/La2O3 CATALYST AND ITS KINETICS STUDY OF HYDROUS HYDRAZINE FOR HYDROGEN GENERATION |
Yujie ZHONG1,Hongbin DAI2( ),Ping WANG2 |
1 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2 Key Laboratory of Advanced Energy Storage Materials of Guangdong Province, School of Materials Science and Engineering, South China University of Technology, Guangzhou 510641, China |
引用本文:
钟玉洁,戴洪斌,王平. 水合肼制氢Ni-Pt/La2O3催化剂研制及其反应动力学研究*[J]. 金属学报, 2016, 52(4): 505-512.
Yujie ZHONG,
Hongbin DAI,
Ping WANG.
PREPARATION OF Ni-Pt/La2O3 CATALYST AND ITS KINETICS STUDY OF HYDROUS HYDRAZINE FOR HYDROGEN GENERATION[J]. Acta Metall Sin, 2016, 52(4): 505-512.
| [1] | Wang P, Kang X D.Dalton Trans, 2008; 40: 5400 | | [2] | Zhu Q L, Xu Q.Energy Environ Sci, 2015; 8: 478 | | [3] | Demirci U B, Miele P.Energy Environ Sci, 2009; 2: 627 | | [4] | Cho S J, Lee J, Lee Y S, Kim D P.Catal Lett, 2006; 109: 3 | | [5] | Singh S K, Zhang X B, Xu Q.J Am Chem Soc, 2009; 131: 9894 | | [6] | He L, Huang Y Q, Wang A Q, Wang X D, Zhang T.AIChE J, 2013; 59: 4297 | | [7] | He L, Liang B L, Li L, Yang X F, Huang Y Q, Wang A Q, Wang X D, Zhang T.ACS Catal, 2015; 5: 1623 | | [8] | He L, Huang Y Q, Wang X D, Chen X W, Delgado J J, Zhang T.Angew Chem Int Ed, 2012; 51: 6191 | | [9] | Singh S K, Xu Q.J Am Chem Soc, 2009; 131: 18032 | | [10] | He L, Huang Y Q, Wang A Q, Lu Y, Liu X Y, Chen X W, Delgado J J, Wang X D, Zhang T.J Catal, 2013; 298: 1 | | [11] | Wen L, Du X Q, Su J, Luo W, Cai P, Cheng G Z.Dalton Trans, 2015; 13: 6212 | | [12] | Singh S K, Singh A K, Aranishi K, Xu Q.J Am Chem Soc, 2011; 133: 19638 | | [13] | Singh S K, Xu Q.Chem Commun, 2010; 46: 6545 | | [14] | Singh A K, Xu Q.ChemCatChem, 2013; 5: 3000 | | [15] | Singh A K, Xu Q.Int J Hydrogen Energy, 2014; 39: 9128 | | [16] | Zhang J J, Kang Q, Yang Z H, Dai H B, Zhuang D W, Wang P.J Mater Chem, 2013; 1A: 11623 | | [17] | Wang H L, Yan J M, Wang Z L, O S I, Jiang Q.J Mater Chem, 2013; 1A: 14957 | | [18] | Wang H L, Yan J M, Li S J, Zhang X W, Jiang Q.J Mater Chem, 2015; 3A: 121 | | [19] | Singh S K, Lu Z H, Xu Q.Eur J Inorg Chem, 2011; (14): 2232 | | [20] | Singh S K, Iizuka Y, Xu Q.Int J Hydrogen Energy, 2011; 36: 11794 | | [21] | Cao N, Su J, Luo W, Cheng G Z.Int J Hydrogen Energy, 2014; 39: 9726 | | [22] | Cao N, Yang L, Du C, Su J, Luo W, Cheng G Z.J Mater Chem, 2014; 2A: 14344 | | [23] | Jiang Y Y, Kang Q, Zhang J J, Dai H B, Wang P.J Power Sources, 2015; 273: 554 | | [24] | Jiang Y Y, Dai H B, Zhong Y J, Chen D M, Wang P.Chem Eur J, 2015; 21: 15439 | | [25] | Zhong Y J, Dai H B, Jiang Y Y, Chen D M, Zhu M, Sun L X, Wang P.J Power Sources, 2015; 300: 294 | | [26] | Wang J, Zhang X B, Wang Z L, Wang L M, Zhang Y.Energy Environ Sci, 2012; 5: 6885 | | [27] | Siegmann H C, Schlapbach L, Brundle C R.Phys Rev Lett, 1978; 40: 972 | | [28] | Nikolla E, Schwank J, Linic S.J Am Chem Soc, 2009; 131: 2747 | | [29] | Holewinski A, Xin H L, Nikolla E, Linic S.Curr Opin Chem Eng, 2013; 2: 312 | | [30] | Zhang Q L, Wu Y, Sun X L, Ortega J.Ind Eng Chem Res, 2007; 46: 1120 | | [31] | Zhang J S, Delgass W N, Fisher T S, Gore J P.J Power Sources, 2007; 164: 772 | | [32] | Zhao B, Song J, Ran R, Shao Z P.Int J Hydrogen Energy, 2012; 37: 1133 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|