					引用本文:
						|  |  
    					|  |  
    					| 晶体相场模拟晶界预熔及熔化 |  
						| 卢艳丽,牧虹,侯华欣,陈铮 |  
					| 西北工业大学凝固技术国家重点实验室, 西安 710072 |  
						|  |  
    					| PHASE FIELD CRYSTAL SIMULATION FOR THE PREMELTING AND MELTING OF GRAIN BOUNDARY |  
						| LU Yanli, MU Hong, HOU Huaxin, CHEN Zheng |  
						| State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072 |  
								卢艳丽,牧虹,侯华欣,陈铮. 晶体相场模拟晶界预熔及熔化[J]. 金属学报, 2013, 49(3): 358-364.	
																												LU Yanli,
																								MU Hong,
																								HOU Huaxin,
																												CHEN Zheng. 
				PHASE FIELD CRYSTAL SIMULATION FOR THE PREMELTING AND MELTING OF GRAIN BOUNDARY[J]. Acta Metall Sin, 2013, 49(3): 358-364.
 
					
						| 
								
									|  
          
          
            
                         
            
									            
									                
																														  
																| [1] Luo J.Crit Rev Solid State Mater Sci, 2007; 32: 67 [2] Straumal B B, Baretzky B.Interface Sci, 2004; 12: 147 [3] Inoko F, Okada T, Muraga T, Nakano Y, Yoshikawa T.Interface Sci, 1997; 4: 263 [4] Alsayed A M, Islam M F, Zhang J, Collings P J, Yodh A G.Science, 2005; 309: 1207 [5] Rappaz M, Jacot A, Boettinger W J.Metall Mater Trans, 2003; 34A: 467 [6] Wang N, Mokadem S, Rappaz M, Kurz W.Acta Mater, 2004; 52: 3173 [7] Suzuki A, Mishin Y.J Mater Sci, 2005; 40: 3155 [8] Olmsted D L, Dorel B, Ari A, Foiles S M, Mark A, Alain K.Phys Rev Lett, 2011; 106: 046101 [9] Luo J, Gupta V K, Yoon D H.Appl Phys Lett, 2005; 87: 231902 [10] Straumal B, Kogtenkova O, Protasova S, Mazilkin A, Zieba P, Czeppe T, Wojewoda-Budka J, Faryna M. Mater Sci Eng, 2008; A495: 126 [11] Keblinski P, Phillpot S R, Wolf D, Gleiter H.Acta Mater, 1997; 41: 631 [12] Tang M, Carter W C, Cannon R M.Phys Rev Lett, 2006; 97: 075502 [13] Kikuchi R, Cahn J W.Phys Rev, 1980; 21: 5 [14] Besold G, Mouritsen O G.Phys Rev, 1994; 50B: 6573 [15] Ramakrishnan T V, Yussouff M.Phys Rev, 1979; 19B: 2775 [16] Elder K R, Katakowski M, Haataja M, Grant M.Phys Rev Lett, 2002; 88: 245701 [17] Elder K R, Grant M.Phys Rev, 2004; 70E: 051605 [18] Goldenfeld N, Athreya B P, Dantzig J A.Phys Rev, 2005; 72E: 020601 [19] Stefanovic P, Haataja M, Provatas N.Phys Rev Lett, 2006; 96: 225504 [20] Berry J, Grant M, Elder K R.Phys Rev, 2006; 73E: 031609 [21] Wu K A, Karma A, Hoyt J J, Asta M.Phys Rev, 2006; 73B: 094101 [22] Wu K A, Karma A.Phys Rev, 2007; 76B: 184107 [23] Elder K R, Provatas N, Berry J, Stefanovic P, Grant M.Phys Rev, 2007; 75B: 064107 [24] Morris J R.Phys Rev, 2002; 66B: 144104 [25] Williams P L, Mishin Y.Acta Mater, 2009; 57: 3786 [26] Von Alfthan S, Kaski K, Sutton A P.Phys Rev, 2007; 76B: 245317 [27] Mellenthin J, Karma A, Plapp M.Phys Rev, 2008; 78B: 184110 |  
             
												
											    	
											        	|  | Viewed |  
											        	|  |  |  
												        |  | Full text 
 | 
 
 |  
												        |  |  |  
												        |  | Abstract 
 | 
 |  
												        |  |  |  
												        |  | Cited |  |  
												        |  |  |  |  
													    |  | Shared |  |  
													    |  |  |  |  
													    |  | Discussed |  |  |  |  |