恒位移下BaTiO3单晶在空气中亚临界裂纹扩展与畴变
赵显武1;褚武扬2;乔利杰2
1.北京大学力学与空天技术系; 北京 100871
2.北京科技大学腐蚀与防护中心; 北京 100083
SUB–CRITICAL CRACK GROWTH IN AIR AND DOMAIN SWITCHING FOR BaTiO3 SINGLE CRYSTAL UNDER CONSTANT DEFLECTION
ZHAO Xianwu 1;CHU Wuyang 2;QIAO Lijie2
1.Department of Mechanics and Aerospace Engineering; Peking University; Beijing 100871
2.Corrosion and Protection Center; University of Science and Technology Beijing; Beijing 100083
引用本文:

赵显武 褚武扬 乔利杰. 恒位移下BaTiO3单晶在空气中亚临界裂纹扩展与畴变[J]. 金属学报, 2010, 46(2): 167-171.
, , . SUB–CRITICAL CRACK GROWTH IN AIR AND DOMAIN SWITCHING FOR BaTiO3 SINGLE CRYSTAL UNDER CONSTANT DEFLECTION[J]. Acta Metall Sin, 2010, 46(2): 167-171.

全文: PDF(2207 KB)  
摘要: 

用正交偏振光显微镜, 通过原位观察研究了恒位移下BaTiO3单晶贯穿裂纹快速扩展与畴变的关系, 以及在室温空气中(湿度为35%RH)亚临界裂纹扩展和畴变的关系. 结果显示, 加载开始时首先出现畴变, 且其体积分数随载荷升高而增大; 当载荷达到临界值时, 裂纹快速形核、扩展并止裂. 在空气中保持恒位移, 畴变能慢慢发生,即空气中水吸附能促进畴变, 当畴变发展到临界条件时就引起裂纹的亚临界扩展(即应力腐蚀).

关键词 : BaTiO3单晶,  畴变,  亚临界裂纹扩展    
Abstract:

BaTiO3 single crystal with superior dielectric, pyroelectric, piezoelectric and electro–optic properties has triggered much attention due to numerous potential applications in microelectronic devices, sensors and micro/nanoelectromechanical systems. However, one of the main disadvantages for BaTiO3 single crystal is that after long–term working under mechanical field or electric field, cracks may be nucleated and propagated. The crack nucleation and propagation in ferroelectric materials are closely related to the domain configurations, and their relationship with crack propagation, nucleation and domain switching, is not known clearly, so it is imperative to take more effort to research this relationship. Here, the relationship of domain switching with crack propagating quickly as well as sub–critical crack growth in ambient air for constant deflection sample of BaTiO3 single crystal has been in situ tudied using a polarized light microscopy. The results indicate that domain switching occurs first and he volume fraction of swiched bnds increases dring loading. When the load reaches to a critical value, crack will be initiaed nd propagated qickly. Keeping the constant deflection, the domain switch could still occur but very slowly, i.e., adsorption of water in air is able to promote domain switchng. As a result of adsorption–enhanced domain switching, cracks are propagated lowly n air, that s say, sub–critical crack growth or stress corrosion cracking in air could occur for BaTiO3 single crystal under constant deflection.

Key words: BaTiO3 single crystal    domain switching    sub–critical crack growth
收稿日期: 2009-04-30     
基金资助:

国家自然科学基金资助项目50632010和50572006

作者简介: 赵显武, 男, 蒙古族, 1967年生, 讲师, 博士

[1] Zhao X W, Chu W Y, Su Y J, Li J X, Gao K W, Qiao L J. Acta Metall Sin, 2006; 42: 13
(赵显武, 褚武扬, 宿彦京, 李金许, 高克玮, 乔利杰. 金属学报, 2006; 42: 13)
[2] Hao T H, Gong X, Suo Z. J Mech Phys Solids, 1996; 44: 23
[3] Jiang B, Bai Y, Chu W Y, Su Y J, Qiao L J. Appl Phys Lett, 2008; 93: 152905
[4] Jiang B, Bai Y, Cao J L, Su Y J, Shi S Q, Chu W Y, Qiao L J. J Appl Phys, 2008; 103: 116102
[5] Yang W, Fang F, Tao M. Int J Solids Struct, 2001; 38: 2203
[6] Busche M J, Hsia K J. Scr Mater, 2001; 44: 207
[7] Fang F, Yang W. Mater Lett, 2002; 57: 198
[8] Kreher W S. J Mech Phys Solids, 2002; 50: 1029
[9] Fang D N, Jiang Y J, Li S, Sun C T. Acta Mater, 2007; 55: 5758
[10] Jiang Y J, Fang D N, Li F X. Appl Phys Lett, 2007; 90: 222907
[11] Wang R M, Chu W Y, Su Y J, Li J X, Qiao L J. Mater Sci Eng, 2006; B135: 141
[12] Fang F, Yang W, Zhang F C. J Am Ceram Soc, 2005; 88:2491
[13] Wang Y, Chu W Y, Gao K W, Su Y J, Qiao L J. Appl Phys Lett, 2003; 82: 1583
[14] Su Y J, Wang Y, Chu W Y, Gao K W, Qiao L J. Acta Mater, 2004; 52: 3713
[15] Wang R M, Chu W Y, Gao K W, Su Y J, Qiao L J. Mater Lett, 2004; 58: 1811
[16] Wang Y, Chu W Y, Su Y J, Qiao L J. Mater Sci Eng, 2002; B95: 263
[17] Micjhalske T A, Freiman S W. J Am Ceram Soc, 1983; 66: 284

[1] 姜冰 郭志猛 邢献然. 外场作用下BaTiO3单晶裂纹扩展和畴变[J]. 金属学报, 2011, 47(5): 605-610.
[2] 赵显武 褚武扬 乔利杰. 垂直电场下BaTiO3单晶的畴变与压痕裂纹的演化[J]. 金属学报, 2010, 46(3): 340-345.
[3] 姜冰; 白杨; 禇武扬; 乔利杰; 宿彦京 . 湿度对恒电场下BaTiO3单晶中畴变的影响[J]. 金属学报, 2008, 44(9): 1090-1094 .
[4] 刘苹莉; 马星桥; 褚武扬; 乔利杰 . PZT铁电陶瓷力电耦合的三维相场模拟[J]. 金属学报, 2008, 44(8): 927-932 .
[5] 钮萼 . 湿空气中恒磁场导致(Tb, Dy)Fe 2合金的滞后开裂[J]. 金属学报, 2006, 42(4): 369-373 .
[6] 张飒; 程璇; 张颖 . 铁电陶瓷畴变的原位Raman谱观测[J]. 金属学报, 2005, 41(6): 663-668 .
[7] 王瑞敏; 褚武扬; 宿彦京; 高克玮; 乔利杰 . 浸蚀促进BaTiO3单晶的畴变和裂纹扩展的研究[J]. 金属学报, 2005, 41(3): 297-301 .
[8] 陈志武; 程璇; 张颖 . Al--Li--Cu--Mg--Zr alloy, fatigue,[J]. 金属学报, 2004, 40(3): 230-234 .
[9] 张颖; 陈志武; 程璇; 张飒 . 原位XRD法研究电疲劳过程中铁电陶瓷PLZT的畴变[J]. 金属学报, 2004, 40(12): 1299-1304 .