| 铬和硅对一种35Ni-15Cr型铁基高温合金力学性能和组织结构的影响 |
| 郭建亭 |
| 中国科学院金属研究所铁基高温合金研究组 |
|
| THE EFFECT OF Cr AND Si ON THE MECHANICAL PROPERTIES AND MICROSTRUCTURE OF AN IRON-BASE ALLOY |
| Res. Gp. of Iron-Base Superalloy(Institute of Metal Research; Academia Sinica) |
引用本文:
郭建亭. 铬和硅对一种35Ni-15Cr型铁基高温合金力学性能和组织结构的影响[J]. 金属学报, 1978, 14(4): 348-461.
.
THE EFFECT OF Cr AND Si ON THE MECHANICAL PROPERTIES AND MICROSTRUCTURE OF AN IRON-BASE ALLOY[J]. Acta Metall Sin, 1978, 14(4): 348-461.
[1] 铁基高温合金研究组,金属学报,14(1978) ,227. [2] Speich, G. R. and Clark, J. B., Precipitation From Iron-base Alloys, Gordon and Breach, New York, 1965, p. 92.{ |
|