| 关于平辊轧制力计算公式 |
| 陈家民 |
| 东北工学院 |
|
| A NEW MATHEMATIC TREATMENT OF ROLLING PRESSURE CALCULATIONS |
| Chen Jia-min(North-East Institute of Technology) |
引用本文:
陈家民. 关于平辊轧制力计算公式[J]. 金属学报, 1978, 14(4): 358-372.
.
A NEW MATHEMATIC TREATMENT OF ROLLING PRESSURE CALCULATIONS[J]. Acta Metall Sin, 1978, 14(4): 358-372.