| 熔锍Cu_2S与氢反应的动力学 |
| 刘纯鹏;郭有根;艾永衡 |
| 昆明工学院;昆明工学院;昆明工学院 |
|
| THE KINETICS OF REACTION OF MOLTEN CUPROUS SULPHIDE WITH HYDROGEN |
| Liu Chun-peng Guo You-gen Ai Yong-heng (Kunming College of Engineering) |
引用本文:
刘纯鹏;郭有根;艾永衡. 熔锍Cu_2S与氢反应的动力学[J]. 金属学报, 1978, 14(4): 373-382.
,
,
.
THE KINETICS OF REACTION OF MOLTEN CUPROUS SULPHIDE WITH HYDROGEN[J]. Acta Metall Sin, 1978, 14(4): 373-382.
[1] Wright, J. H. et al., Met. Trans., 245 (1972) , 1749. [2] Small, W. M. et al., Met. Trans., 4 (1973) , 2045. [3] Byerley, J. J. et al., Met. Trans., 4 (1973) , 1507. [4] Aynsley, E. E. et al., Quart. J. Chem. Sco., London, (1935) , 65. [5] Schuhmann, R. Jr. and Moles, O. W., Trans. Amer. Inst. Mining Met. Eng., 191 (1951) , 235. [6] 柳喬哲夫,日本鉱業会誌,78(1962) ,№ 883(1) ,43. |
|