| 硼析出相与壳层状硼脆断口——中碳含硼结构钢脆化机理的讨论 |
| 刘富有 |
| 昆明钢铁公司中心试验室 |
|
| SHELL-SHAPED FRACTURE IN A MEDIUM CARBON STEEL DUE TO BORON EMBRITTLEMENT |
| Liu Fuyu Central Laboratory of Kunming Iron and Steel Company |
引用本文:
刘富有. 硼析出相与壳层状硼脆断口——中碳含硼结构钢脆化机理的讨论[J]. 金属学报, 1979, 15(3): 373-460.
.
SHELL-SHAPED FRACTURE IN A MEDIUM CARBON STEEL DUE TO BORON EMBRITTLEMENT[J]. Acta Metall Sin, 1979, 15(3): 373-460.
[1] Brown, A. et al., Metal Sci. J., 8 (1974) , 317. [2] Ueno, M. and Inoue, J., Trans. Iron Steel Inst. Jap., 13 (1973) , 210. [3] Brewer, L. and Chang, S. G., Metals Handbook, Vol. 8, ASM, 1973. p. 400. |
|