Pb,Mg对压铸锌合金长期时效性能的影响
王佐臣
中国科学院长春光学精密机械研究所
EFFECTS OF Pb AND Mg ON THE PROPERTIES OF LONG TERM AGING Zn-4Al ALLOY
Wang Zuochen Changchun Institute of Optical and Fine Machines; Academia Sinica
引用本文:

王佐臣. Pb,Mg对压铸锌合金长期时效性能的影响[J]. 金属学报, 1980, 16(3): 349-379.
. EFFECTS OF Pb AND Mg ON THE PROPERTIES OF LONG TERM AGING Zn-4Al ALLOY[J]. Acta Metall Sin, 1980, 16(3): 349-379.

全文: PDF(1709 KB)  
摘要: <正> 压铸锌合金性能的老化现象,与所含杂质(如Pb,Sn,Cd)及合金在常温下的相变有关。 曾取三种压铸锌合金〔Zn-4Al-0.05Mg,Zn-4Al-2.7Cu-0.05Mg和Zn-4Al-1Cu-0.05Mg〕,观察不同含Pb量对长期时效后合金性能的影响。
Abstract:Tests were made of the effects of Pb and Mg on the property changes ofZn-4Al alloy in 20 years natural aging. It appears to that Pb is favourable tothe phase transformation of alloy which is remarkably caused its volume change.Mg dissloves in the Zn alloy with in its certain maximum solubility only. Thisseems to be independent of Pb contaminated. The optimum addition of Mg maythen be chosen properly. Furthermore, the influence of presence of Cu was alsodiscussed.