| Pb,Mg对压铸锌合金长期时效性能的影响 |
| 王佐臣 |
| 中国科学院长春光学精密机械研究所 |
|
| EFFECTS OF Pb AND Mg ON THE PROPERTIES OF LONG TERM AGING Zn-4Al ALLOY |
| Wang Zuochen Changchun Institute of Optical and Fine Machines; Academia Sinica |
引用本文:
王佐臣. Pb,Mg对压铸锌合金长期时效性能的影响[J]. 金属学报, 1980, 16(3): 349-379.
.
EFFECTS OF Pb AND Mg ON THE PROPERTIES OF LONG TERM AGING Zn-4Al ALLOY[J]. Acta Metall Sin, 1980, 16(3): 349-379.
|